SIKAFLEX 715

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SIKAFLEX 715

Main features

  • Semi-Self-Leveling Roof Application
  • 30-Minute Skin Time
  • 500% Cured Elongation

Product Description

Sikaflex-715 is a one-component, moisture-curing silane-terminated polymer sealant with semi-self-leveling flow for roof sealing. The white or black material has a 30-minute skin time at 23 deg C and 50% relative humidity and can be applied from 5 to 40 deg C. After cure, it provides 500% elongation, 0.6 MPa tensile strength, and a service temperature range of -50 to 90 deg C. It seals RV roofing components and repair areas involving EPDM, metals, coatings, ceramics, and plastics, with substrate preparation and compatibility verified for the specific assembly.

Key features

  • Semi-self-leveling flow: Controls placement across horizontal roof joints and repair areas
  • 500% cured elongation: Typical ASTM D412 value for the cured sealant
  • Very good UV resistance: Supports exposed roof joints within the documented application scope

Applications

Sealing and repair of roof-membrane joints, seams, and penetrations; RV and specialty-vehicle roofing components using the published preparation procedure.

Technical Specifications

General Properties
Chemistry Type
Silane Terminated Polymer
Color
The color
white, black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
one
Density
Volumetric mass per unit
1.52 kg/m3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Thermal Properties
Operating Temperature
-50 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base Silane Terminated Polymer As supplied
Color White, black CQP001-1
Density 1.52 kg/l Uncured
Flow behavior Semi self-leveling As supplied
Application temperature 5 to 40 deg C Product and substrate process range
Skin time 30 minutes CQP019-1; 23 deg C / 50% RH
Shelf life 9 months Cartridge; storage below 25 deg C
Shelf life 6 months Drum; storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 10 Shore A CQP023-1 / ISO 48-4
Tensile strength 0.6 MPa ASTM D412
Elongation at break 500 % ASTM D412
Service temperature -50 to 90 deg C CQP513-1

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers