SIKAFLEX 295UV

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

SIKAFLEX 295UV

Main features

  • Organic-Glass Marine Bonding
  • Weather-Resistant Exterior Sealing
  • Defined 45-Minute Open Time

Product Description

Sikaflex-295 UV is a paste-like, one-component moisture-curing polyurethane adhesive and sealant for marine glazing. The non-sag material is available in black or white and provides a 45-minute open time at 23 deg C and 50% relative humidity. After cure, typical properties include 500% elongation, 2 MPa tensile strength, and 5 N/mm tear propagation resistance under ISO 527 and ISO 34. It bonds and seals plastic glazing materials such as polycarbonate and PMMA in boats and ships and is also used for exposed marine joints where aging and weathering resistance are required.

Key features

  • Organic-glass bonding: Suitable glazing materials include polycarbonate and PMMA
  • Weathering-resistant seal: The adhesive sealant is used for exposed marine joints
  • 45-minute open time: Defines the installation window at 23 deg C and 50% relative humidity

Applications

Bonding and sealing plastic glazing materials in boats and ships; interior and exterior marine sealing; exposed marine joints.

Product Family

SIKAFLEX 295UV

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Color
The color
black,white
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
one
Density
Volumetric mass per unit
1.3 kg/m3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Thermal Properties
Operating Temperature
-50 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color Black, white CQP001-1
Density 1.3 kg/l Uncured
Non-sag properties Good As supplied
Application temperature 10 to 35 deg C Product and ambient range
Skin time 60 minutes CQP019-1; 23 deg C / 50% RH
Open time 45 minutes CQP526-1; 23 deg C / 50% RH
Shelf life 12 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Shrinkage 1 % CQP014-1
Hardness 35 Shore A CQP023-1 / ISO 48-4
Tensile strength 2 MPa CQP036-1 / ISO 527
Elongation at break 500 % CQP036-1 / ISO 527
Tear propagation resistance 5 N/mm CQP045-1 / ISO 34
Service temperature -50 to 90 deg C CQP509-1 / CQP513-1

Leading Brands Trust in Our Products and Services