SIKAFAST 3131S

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

SIKAFAST 3131S

Main features

  • Seven-Minute Open Time
  • Built-In Bondline Spacing
  • High-Strength Concealed-Joint Bonding

Product Description

SikaFast-3131 S combines a fast-curing, two-component methacrylate adhesive with 0.68 to 0.84 mm spacer shims for controlled bond thickness. The 10:1 volume-mix thixotropic paste has a seven-minute open time at 23 deg C and 50% relative humidity, supporting quick assembly and fixturing. After cure, typical properties include 9 MPa tensile strength, 50% elongation, and 10.5 MPa tensile lap-shear strength under ASTM D638 and CQP046-6 / ISO 4587. It is used for high-strength fastening of concealed joints on aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers and can replace or complement mechanical fixation.

Key features

  • Built-in spacer shims: 0.68 to 0.84 mm shims maintain a uniform bond thickness
  • Seven-minute open time: Supports quick assembly at 23 deg C and 50% relative humidity
  • Structural bond strength: Typical tensile lap-shear strength is 10.5 MPa under CQP046-6 / ISO 4587

Applications

High-strength fastening of concealed joints; bonding aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers; replacing or complementing rivets, screws, or welding.

Technical Specifications

General Properties
Chemistry Type
Methacrylate
Color
The color
Straw
Density (g)
0.99 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
50 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for SikaFast-3131 S Part A, SikaFast-3081 N Part B, and the mixed adhesive system.

Property Value Unit Method / condition
Part A density 0.96 kg/l SikaFast-3131 S Part A
Part B density 1.30 kg/l SikaFast-3081 N Part B
Mixed density 0.99 kg/l Calculated mixed value
Mix ratio by volume 10:1 Part A:Part B
Consistency Thixotropic paste Mixed adhesive
Spacer shim thickness 0.68 to 0.84 mm Incorporated spacers
Application temperature 10 to 35 deg C Substrate and adhesive range
Open time 7 minutes CQP526-2; 23 deg C / 50% RH
Technical properties

After-processing / final-state properties

Typical cured values for the mixed adhesive system.

Property Value Unit Method / condition
Hardness 65 Shore D CQP023-1 / ISO 48-4
Tensile strength 9 MPa ASTM D638
Elongation at break 50 % ASTM D638
E-modulus at 0-5% elongation 100 MPa ASTM D638
Tensile lap-shear strength 10.5 MPa CQP046-6 / ISO 4587
Service temperature -30 to 80 deg C CQP513-1