ROYAL HYDRA FAST-EN DC12623

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ROYAL HYDRA FAST-EN DC12623

Main features

  • One-part waterborne spray format
  • Wet or dry mating
  • Soft supple adhesive layer

Product Description

H.B. Fuller Hydra FAST-EN DC12623 Contact Adhesive is a one-part waterborne spray contact adhesive for bonding porous materials, particularly open-cell polyurethane foam. The adhesive supports either wet mating or dry mating, allowing the assembly sequence to be matched to the substrate and production method. Its sprayable form supports controlled coverage across porous surfaces, while the finished adhesive layer remains soft and supple rather than forming a rigid joint. DC12623 is suited to contact-bonding processes where flexible handling and supported wet- or dry-mating options are important.

Key features

  • One-part waterborne format: Requires no component mixing before spray application
  • Wet or dry mating: Supports either documented contact-bonding sequence
  • Soft, supple bond: Maintains a flexible adhesive layer after mating

Applications

Bonding porous materials, particularly open-cell polyurethane foam, by supported wet-mating or dry-mating contact-adhesive processes.

Product Family

ROYAL HYDRA FAST-EN DC12623

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White when wet
Chemistry Type
1-part, water-based natural rubber contact adhesive
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.942

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product form One-part waterborne contact adhesive - As supplied
Application method Spray - Applied to porous bonding surfaces
Mating process Wet or dry mating - Select the documented contact-bonding sequence
Target materials Porous materials; open-cell polyurethane foam - Documented application scope