ROYAL DOUBLE BUBBLE 04001

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04001

Main features

  • Fast 15-to-30-Minute Handling
  • Premeasured 1:1 Packet Mixing
  • High-Cohesion Structural Repair

Product Description

Hardman Double/Bubble 04001 Extra Fast-Set Epoxy is a 3.5 g premeasured, two-part epoxy packet for fast structural bonding, fixturing, patching, and repair. The amber liquid mixes at 1:1 by volume and has a 3 to 5 minute gel time at 25 deg C, followed by 15 to 30 minute handling time and full cure in 24 hours at 23 deg C. Typical cured data include 3,000 psi overlap shear strength on acid-etched aluminum at 25 deg C and 80 Shore D hardness. The grade bonds metals, wood, concrete, ceramics, stone, glass, leather, and many plastics.

Key features

  • Premeasured 1:1 packet: The 3.5 g dual pouch keeps the two components portioned for one-shot mixing.
  • Fast handling: Handling strength develops in 15 to 30 minutes at room temperature.
  • Cured structural strength: Typical overlap shear strength is 3,000 psi on acid-etched aluminum at 25 deg C.

Applications

Applications include fast bonding, patching, fixturing, and repair of metal, ceramics, glass, wood, concrete, stone, leather, and selected plastics.

Product Family

ROYAL DOUBLE BUBBLE 04001

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
82 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
Volume mix ratio1:1-Part A to Part B
Mixed viscosity40,000cPAt 25 deg C
Gel time3-5minAt 25 deg C; 4 g mixed mass
Handling time15-30minRoom-temperature cure
Full cure24hAt 23 deg C
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness80Shore DASTM D2240
Tensile strength7,250psiASTM D638
Elongation at break8.5%ASTM D638
Overlap shear strength3,000psiAcid-etched aluminum; ASTM D1002; 25 deg C and 50% RH
T-peel strength1.8pliAcid-etched aluminum-to-aluminum; 25 deg C
Operating temperature82deg CCured adhesive