PERMABOND QFS16

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND QFS16

Main features

  • 5-Second Steel Set Time
  • Faster Cure Through Gaps
  • Reduced Plastic Stress Cracking

Product Description

Permabond QFS16 is a colorless cyanoacrylate activator for shortening set time on closely mated parts, porous surfaces, gaps, and wire-tacking assemblies. It is applied to one component by wiping, spraying, or dipping and allowed to evaporate before adhesive is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. The formulation also reduces stress cracking, surface discoloration, and adhesive frosting on supported plastic parts.

Key features

  • Rapid Steel Set: Provides a typical 5-second set on gap-free steel under stated conditions.
  • Gap and Porous-Surface Cure: Accelerates cyanoacrylate cure through gaps and on porous materials.
  • Reduced Plastic Surface Effects: Helps limit stress cracking, discoloration, and frosting on supported plastics.

Applications

Applications include porous or poorly mated parts, gap bonding, wire tacking, excess-fillet cure, and supported plastic assemblies.

Technical Specifications

General Properties
Color
The color
Colorless
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.68
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-2 °C
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product typeCyanoacrylate activatorAs supplied
ColorColorlessAs supplied
Specific gravity0.68As supplied
Flash point-2deg CAs supplied
Application methodWipe, spray, or dip one componentAllow full evaporation before bonding
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.

Property Value Unit Method / condition
Set time - steel, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, 5 mil gap40-60secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, no gap, control10-15secondsAt 23 deg C without QFS16
Set time - Buna-N, no gap10secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - phenolic, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16