PERMABOND QFS10

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND QFS10

Main features

  • 5-Second Steel Set Time
  • Faster Cure Through Gaps
  • Porous Surface Activation

Product Description

Permabond QFS10 is a water-white cyanoacrylate activator that accelerates set on porous or poorly mated parts and through sizable gaps. Applied by wiping, spraying, or dipping one component, it must evaporate before cyanoacrylate is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. QFS10 also supports wire tacking, post-application curing of excess fillets, and reduced frosting or fogging on supported assemblies.

Key features

  • Faster Gap Cure: Accelerates cyanoacrylate set through poorly mated joints and sizable gaps.
  • Porous Surface Activation: Limits adhesive soak-in before cure on porous materials.
  • Post-Application Activation: May be sprayed or dripped onto excess fillets and wire-tacking joints.

Applications

Applications include porous-part bonding, poorly mated joints, wire tacking, excess-fillet cure, and supported plastic assemblies.

Technical Specifications

General Properties
Color
The color
Water-white
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-4.4 °C
Other Properties
Storage Temperature
5-25 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product typeCyanoacrylate activatorAs supplied
ColorWater-whiteAs supplied
Flash point-4.4deg CAs supplied
Application methodWipe, spray, or dip one componentAllow full evaporation before bonding
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.

Property Value Unit Method / condition
Set time - steel, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10
Set time - steel, 5 mil gap40-60secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10
Set time - steel, no gap, control10-15secondsAt 23 deg C without QFS10
Set time - Buna-N, no gap10secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10
Set time - phenolic, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers