OPTOLINQ LE-8011HT | Two part epoxy resin

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OPTOLINQ LE-8011HT | Two part epoxy resin

Main features

  • Excellent thermal stability
  • Excellent UV stability
  • High light transmittance

Product Description

OPTOLINQ LE-8011HT is an epoxy resin specifically designed for infrared device packaging applications. This resin exhibits superior thermal stability and excellent UV stability, ensuring that devices can withstand high temperatures and ultraviolet light exposure without degradation.

Upon curing, OPTOLINQ LE-8011HT forms robust cross-linked networks, providing strong adhesion and maintaining airtight seals. These properties make LE-8011HT an ideal high-performance and High Transmittance solution for IR device packaging. LE-8011HT delivers comparable optical functionality as Loctite Stycast OS4000 with AC 7115 dye. 

Key Features

  • Designed for Optoelectronic Device Packaging: effectively seals and protects optoelectronic components.
  • Superior Thermal Stability: LE-8011U can withstand high temperatures without degrading.
  • Excellent UV Stability: Resistant to damage and degradation from exposure to ultraviolet light.
  • High Optical Clarity: Delivers exceptional light transmission, critical for optoelectronic device functionality.
  • Strong Adhesion: Provides excellent bonding strength to diverse substrates, enhancing package reliability.
  • Enhanced Air Tightness: Offers effective barrier properties, minimizing gas permeation and protecting sensitive components.

Available versions

 

 

Technical Specifications

General Properties
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:95
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
7 hours
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.51
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.15
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
163-173 °C
Chemical Properties
Moisture absorption
0.74 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
400-800 mPa.s

Additional Information

To meet higher application requirements, liquid encapsulation is expected to have (1) excellent thermal stability; (2) low transmittance decay. Our resin technology could help meet these challenges. With the resin improved in LE-8011HT, the pot life increased (~7 hours), and viscosity decreased (~400-800 cP). LE-8011HT is a Visible light-blocking encapsulation based on the optically clear version LE-8011U product platform, both products remain with superior anti-blue decay and thermal aging stability. Worth to be mentioned, the properties of both products remains within the same range, apart from their appearance in color and optical performance. 

OPTOLINQ LE-8011HT | Visible Light Blocking

LE-8011HT is developed based on LE-8011U, thus LE-8011HT keeps UV-blocking properties as LE-8011U.

OPTOLINQ LE-8011U | Optically Clear-UV Light Blocking 

Optically clear encapsulation with stable UV blocking capabilities.


VisibleLightBlockingEncapsulant_LE8011HT
 OPTOLINQLE-8011UOpticallyclearUVblocking
 

LE-8011U | UV Aging Performance

LE-8011HT has superior anti-blue decay properties as LE-8011U. 

LE-8011U | Thermal Aging Performance

Optically clear encapsulation with stable UV blocking capabilities.

OPTOLINQLE-8011UUVagingperformance

OPTOLINQLE-8011Uthermalagingperformance

 

Processing Instructions

  1. Mix components A and B in a 100:95 weight ratio and stir uniformly. Ensure that the mixture is uniform and free from streaks or unevenness.
  2. Defoam the mixture under vacuum conditions for 5 minutes.  
  3. Recommended curing condition: First cure at 130 °C for 1 hour, then post cure at  150 °C for 4 hours.

Curing conditions should be determined according to the specific needs of the package being encapsulated, the conditions mentioned are for reference only.

 

Storage and Handling

The uncured resin can be cleaned with acetone or a suitable cleaning agent. Water cannot be used as cleaning agent.

Store in a cold, dry, and clean environment between 10–30 °C with relative humidity below 70%. Keep away from exposure to direct sunlight. It is strictly forbidden to store in outdoor environments. At proper storage conditions, unopened Part A and Part B have a shelf life of 12 months. 

 