MOLYKOTE TP-42

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE TP-42

Main features

  • 3,000 N Four-Ball Weld Load
  • Water-Resistant Grease Lubrication
  • Stick-Slip, Galling, and Corrosion Protection

Product Description

MOLYKOTE® TP-42 Paste is a light-beige, adhesive grease-paste for heavily loaded metallic sliding surfaces. Its mineral- and synthetic-oil carrier system combines lithium soap, solid lubricants, and an adhesion improver to support lubrication where water or metal-machining emulsions may be present. The NLGI Grade 2 paste is used primarily for chucks and clamping elements on metal-processing machines, as well as assembly, run-in, spindle, bearing, bushing, sleeve, slide, guide, and track applications. It provides high load-carrying capacity, resistance to washout, corrosion and galling protection, and stick-slip control.

Key features

  • High load-carrying capacity: Provides a typical four-ball weld load of 3,000 N and an Almen-Wieland OK load of 20,000 N.
  • High adhesion: Contains an adhesion improver to help retain the paste on metallic sliding surfaces.
  • Washout resistance: Resists removal by water and metal-machining emulsions.
  • Stick-slip control: Supports smoother movement in slow-speed sliding contacts.
  • Galling and wear protection: Protects highly loaded metallic contacts during sliding and adjustment.
  • Corrosion protection: Provides a typical SKF-Emcor corrosion rating of 0–1.

Applications / Suitable for

  • Chucks and clamping elements on metal-processing machines
  • Sliding surfaces exposed to high contact pressures
  • Machining spindles
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Assembly and run-in lubrication

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Adhesive grease-paste for metallic sliding contacts; NLGI 2
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.19 g/mL at 20°C
Thermal Properties
Operating Temperature
−25°C to 250°C for the solid-lubricant system °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® TP-42 Paste. Values are not intended as specification limits.

Property Value Unit Method / condition
Product type Adhesive grease-paste — For metallic friction combinations
Carrier system Mineral oil and synthetic oil — Supplier-listed composition
Thickener Lithium soap — Supplier-listed composition
Solid lubricant system White solid lubricants — Specific solids not identified in the TDS
Color Light beige — Typical property
NLGI grade 2 — Supplier product classification
Unworked penetration 265–300 0.1 mm ISO 2137
Density 1.19 g/mL ISO 2811 at 20°C
Usable life 60 months Original unopened container stored at or below 20°C
Technical properties

After-application / in-service properties

Typical performance characteristics of the applied paste under the stated laboratory conditions.

Property Value Unit Method / condition
Service-temperature range −25 to 250 °C Thermal stability of the solid-lubricant system
Drop point 125 °C ISO 2176; not a maximum service-temperature rating
Four-ball weld load 3,000 N DIN 51350-4
Four-ball wear scar 0.9 mm DIN 51350-5 under 800 N load
Almen-Wieland OK load 20,000 N Friction force: 1,710 N
Coefficient of friction 0.09 µ Press-fit test
Water resistance 2-90 — DIN 51807-1, static water-resistance rating
Corrosion protection 0–1 — DIN 51802, SKF-Emcor degree of corrosion
Oil separation 1.5 % DIN 51817 standard test