MOLYKOTE M-77

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE M-77

Main features

  • Up to 400 deg C Service
  • Silicone Carrier Oil
  • Selected Metal, Plastic, Rubber, and Elastomer Contacts

Product Description

MOLYKOTE® M-77 Paste is a black-gray solid-lubricant paste based on polyphenylmethyl siloxane oil, lithium soap, and molybdenum disulfide. It is intended for low-speed lubrication points operating under low to moderate loads, including applications exposed to water and extreme temperatures. The paste provides lubrication from −45°C to 230°C. Above 230°C, the silicone carrier volatilizes and the remaining dry lubricating film supports operation up to 400°C. The mineral-oil-free formulation is also suitable for selected elastomer and plastic components, subject to compatibility testing.

Key features

  • Wide temperature capability: Provides paste lubrication from −45°C to 230°C and dry-film lubrication up to 400°C.
  • Silicone carrier oil: Suitable for selected materials that are not resistant to mineral oils.
  • Solid-lubricant protection: Contains molybdenum disulfide to maintain lubrication after the carrier volatilizes.
  • Water resistance: Supports lubrication points exposed to water and moisture.
  • Low-speed performance: Formulated for low-speed contacts under low to moderate loads.
  • Flexible application: Can be applied by brush, spatula, grease gun, automatic lubricator, or compatible central lubrication system.

Applications / Suitable for

  • Metal-to-metal friction and contact surfaces
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Selected plastic, rubber, and elastomer components
  • Brake anchor plates and disc-brake pistons
  • Low-speed lubrication points exposed to water or extreme temperatures

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Solid-lubricant paste; NLGI 2
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.95 g/mL at 20°C
Thermal Properties
Operating Temperature
−45°C to 230°C as paste; dry solid-lubricant film up to 400°C °C

Additional Information

MOLYKOTE® M-77 Paste is a black-gray solid-lubricant paste based on polyphenylmethyl siloxane oil, lithium soap, and molybdenum disulfide. It is intended for low-speed lubrication points operating under low to moderate loads, including applications exposed to water and extreme temperatures. The paste provides lubrication from −45°C to 230°C. Above 230°C, the silicone carrier volatilizes and the remaining dry lubricating film supports operation up to 400°C. The mineral-oil-free formulation is also suitable for selected elastomer and plastic components, subject to compatibility testing.

Key features

  • Wide temperature capability: Provides paste lubrication from −45°C to 230°C and dry-film lubrication up to 400°C.
  • Silicone carrier oil: Suitable for selected materials that are not resistant to mineral oils.
  • Solid-lubricant protection: Contains molybdenum disulfide to maintain lubrication after the carrier volatilizes.
  • Water resistance: Supports lubrication points exposed to water and moisture.
  • Low-speed performance: Formulated for low-speed contacts under low to moderate loads.
  • Flexible application: Can be applied by brush, spatula, grease gun, automatic lubricator, or compatible central lubrication system.

Applications / Suitable for

  • Metal-to-metal friction and contact surfaces
  • Plain bearings, bushings, and sleeves
  • Slides, guides, and tracks
  • Selected plastic, rubber, and elastomer components
  • Brake anchor plates and disc-brake pistons
  • Low-speed lubrication points exposed to water or extreme temperatures
Technical properties

After-application / in-service properties

Typical performance characteristics relevant to the applied paste and remaining dry lubricating film.

Property Value Unit Method / condition
Paste lubrication temperature range −45 to 230 °C Paste-like lubricating state
Dry-film temperature capability Up to 400 °C After carrier volatilization above 230°C
Four-ball weld load 2,000 N DIN 51350-4
Water resistance Good — Supplier-listed qualitative performance benefit
Carrier volatilization Leaves virtually no residue — At temperatures above 230°C; dry sliding film remains
Plastic and elastomer compatibility Compatible with many types — Compatibility testing required before use