MOLYKOTE LONGTERM 2 PLUS

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE LONGTERM 2 PLUS

Main features

  • 3,800 N Four-Ball Weld Load
  • Heavily Loaded Metal-to-Metal Components Protection
  • 25 to 110 deg C Service Range

Product Description

MOLYKOTE® Longterm 2 Plus Extreme Pressure Bearing Grease is a black, mineral-oil-based, lithium-soap grease for highly loaded metal-to-metal components operating at slow to medium-fast speeds. The NLGI Grade 2 formulation contains solid lubricants and extreme-pressure additives that provide wear protection under mixed-friction conditions. It is designed for long-term lubrication of bearings, spline profiles, clutches, guides, slides, and power screw drives, including equipment exposed to moisture, fretting corrosion, or groove formation. The grease can be applied manually or through compatible central lubrication systems and has a normal service-temperature range of −25°C to 110°C.

Key features

  • High load-carrying capacity: Provides a typical four-ball weld load of 3,800 N.
  • Mixed-friction wear protection: Uses solid lubricants and extreme-pressure additives to protect loaded metal contacts.
  • Long-term lubrication: Formulated for extended lubrication of suitable components and operating conditions.
  • Good adhesion: Contains an adhesion improver to help retain the grease on lubricated surfaces.
  • Corrosion and fretting protection: Suitable for components exposed to moisture or oscillating contact.
  • Central-system application: Can be applied by brush, spatula, automatic lubrication device, or compatible central lubrication system.

Applications / Suitable for

  • Rolling-element and plain bearings
  • Spline profiles and clutches
  • Slides, guides, tracks, bushings, and sleeves
  • Power screw drives
  • Motor vehicles, tractors, cranes, earth-moving machinery, conveyors, and forklift trucks
  • Components exposed to moisture, fretting corrosion, or groove formation

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Extreme-pressure bearing grease; NLGI 2
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.9 g/mL at 20°C
Thermal Properties
Operating Temperature
−25°C to 110°C; short exposure up to 130°C is separately qualified °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics of MOLYKOTE® Longterm 2 Plus Extreme Pressure Bearing Grease. Values are not intended as specification limits.

Property Value Unit Method / condition
Base-oil technology Mineral oil — Supplier-listed composition
Thickener Lithium soap — Supplier-listed composition
Solid lubricants MoS2 and graphite — Current DuPont product details
Color Black — Typical property
NLGI consistency class 2 — DIN 51818
Worked penetration 265–295 0.1 mm ISO 2137
Density 0.9 g/mL ISO 2811 at 20°C
Base-oil viscosity 265 mm²/s DIN 51562 at 40°C; calculated base-oil-mixture value
Usable life 60 months Original unopened container stored between 0°C and 40°C
Technical properties

After-application / in-service properties

Typical performance characteristics of the applied grease under the stated laboratory conditions.

Property Value Unit Method / condition
Service-temperature range −25 to 110 °C Short periods up to 130°C
Drop point ≥175 °C ISO 2176
Four-ball weld load 3,800 N DIN 51350-4
Four-ball wear scar 1.0 mm DIN 51350-5 under 800 N load
Almen-Wieland OK load 20,000 N Frictional force at OK load: 3,200 N
FAG FE9 bearing life, F50 100 h DIN 51821-02-A; FE9, 4500/6000-110
DN value 250,000 mm/min Supplier-listed speed characteristic
Oxidation resistance 0.3 bar DIN 51808; pressure drop after 100 h at 99°C
Corrosion protection 0–1 — DIN 51802, SKF-Emcor degree of corrosion
Oil separation 1.7 % DIN 51817 standard test

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers