MOLYKOTE G-N METAL ASSEMBLY PASTE

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-N METAL ASSEMBLY PASTE

Main features

  • Heavy-Duty Assembly Paste
  • 0.08 Coefficient of Friction
  • Metal Interfaces Protection

Product Description

MOLYKOTE® G-N Metal Assembly Paste is a multipurpose, heavy-duty lubricating paste containing molybdenum disulfide and white solid lubricants dispersed in mineral oil. Developed for metal surfaces subjected to extreme pressure and boundary-lubrication conditions, it provides a low coefficient of friction and helps reduce wear, galling, seizing and surface damage during assembly, running-in and maintenance. The paste also helps protect metal interfaces against fretting wear, corrosion and cold welding. It can be applied as a thin film to clean surfaces by burnishing with a lint-free cloth or brushing with short, stiff bristles.

Key features

  • Extreme-pressure lubrication: Lubricates metal surfaces under high-load and boundary-lubrication conditions, with a typical four-ball weld load of 499 kg (1,100 lb).
  • Low-friction performance: Provides a typical coefficient of friction of 0.08 in the CTM 0394 LFW-4 press-fit test.
  • Metal interface protection: Helps reduce galling, seizing, fretting wear, corrosion and cold welding during assembly, running-in and maintenance.

Applications / Suitable for

  • Running-in lubrication of gears, splines, journal bearings, cams and ways
  • Assembly and disassembly of threaded fasteners
  • Press fitting and interference fitting of metal components
  • Bearing shafts, bushings and splines exposed to fretting or cold welding
  • Metalworking operations including machining, stamping, drawing, tube bending, thread rolling, cold heading, swaging and forging

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
buttery, grainy
Color
The color
gray-black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.33

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of MOLYKOTE® G-N Metal Assembly Paste in its as-supplied condition. Values are not intended for preparing specifications.

Property Value Unit Method / condition
Appearance Buttery, grainy paste — Typical
Color Gray–black — Typical
Consistency, penetration, unworked 300 mm/10 CTM 0300
Usable life 60 months From date of manufacture when stored at 32°F to 104°F (0°C to 40°C)
Technical properties

After-processing / final-state properties

Typical lubrication and in-use performance data. Values are not intended for preparing specifications and should not be used alone as the basis of design.

Property Value Unit Method / condition
Approximate service temperature range, solid lubricant 0 to 750 (-18 to 399) °F (°C) Solid-lubricant operating range
Approximate service temperature range, base oil 0 to 250 (-18 to 121) °F (°C) Base-oil operating range
Coefficient of friction 0.08 — CTM 0394; LFW-4 press-fit test, steel versus steel, velocity 0.6 in/min, 10,000 psi, room temperature
Four-ball wear scar 0.76 mm CTM 0351; 80 kg, 1 hour, 1,200 rpm, steel versus steel
Four-ball weld load 499 (1,100) kg (lb) Four-ball weld-load test
Effect on copper strip #1, no discoloration — CTM 0172; after 2 hours at 212°F (100°C)

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers