MOLYKOTE EM-D110 GREASE

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE EM-D110 GREASE

Main features

  • Compatible with Most Plastics
  • High-Viscosity PAO Oil
  • Silicone-Free Lubrication Formulation

Product Description

MOLYKOTE® EM-D110 Grease is a white, high-viscosity-base-oil polyalphaolefin grease developed for lubricating plastic components. Its lithium-soap-thickened formulation contains PTFE and other solid lubricants and is compatible with most plastics. The grease is designed for applications requiring noise reduction and damping, including plastic gears and driveshaft spline connections, while its low seepage supports use where cleanliness is important.

Key features

  • Plastic-component lubrication: Compatible with most plastics and formulated to reduce noise from plastic gears.
  • Noise and vibration damping: High-viscosity base oil supports applications where noise reduction and damping are required.
  • Low-seepage, silicone-free formulation: Supports cleaner application areas and avoids silicone-related contact-point failures.

Applications / Suitable for

  • Plastic gears requiring reduced operating noise
  • Driveshaft spline connections requiring reduced engagement feedback
  • Plastic-component lubrication where damping and low seepage are desired

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White
Density
Volumetric mass per unit
860 kg/m3
Thermal Properties
Operating Temperature
-10 to 150 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the grease as supplied. These values are not intended for use as specification limits.

Property Value Unit Method / condition
Appearance White — Typical
Base oil viscosity 9,850 mm²/s 40°C
Worked penetration 360 — JIS K 2220; worked 60 times
NLGI class 0 to 1 — Typical
Density 0.86 g/cm³ Typical
Drop point 195 °C JIS K 2220
Bleed 2.5 % JIS K 2220; 100°C, 24 hours
Evaporation 0.2 % JIS K 2220; 99°C, 22 hours