MOLYKOTE 3451 Chemical Resistant Bearing Grease

Harmonization Code : 2710199990 |

MOLYKOTE 3451 Chemical Resistant Bearing Grease

Main features

  • Fluorosilicone Grease Formulation
  • 40 to 450 deg F Service Range
  • 340 kg Four-Ball Weld Load

Product Description

MOLYKOTE® 3451 Chemical Resistant Bearing Grease is an NLGI Grade 2 fluorosilicone grease formulated with fluorosilicone oil and fluorinated polymer thickeners for anti-friction bearing lubrication. It combines resistance to many chemicals, fuels, oils, solvents, low-pressure steam, and condensate with load-carrying performance across varying bearing speeds and loads. The grease has an estimated service temperature range of -40 to 450°F (-40 to 232°C) and a maximum estimated Dn value of 200,000. It is intended for bearings and processing equipment operating under demanding chemical, temperature, speed, or load conditions.

Key features

  • Chemical-resistant fluorosilicone formulation: Resists deterioration and washout from many solvents, acids, chlorides, fuels, oils, water, low-pressure steam, and condensate.
  • Wide estimated service temperature range: Supports bearing lubrication from -40 to 450°F (-40 to 232°C), depending on the application environment.
  • Load- and speed-capable bearing grease: Provides a typical ASTM D2596 4-ball weld load of 340 kg and a maximum estimated Dn value of 200,000.

Applications / Suitable for

  • Chemical mixers and pumps
  • Needle bearings in circuit breakers
  • Processing equipment
  • Fuel- and solvent-handling equipment
  • Sealed-for-life bearings operating at high speeds, heavy loads, or high and low temperatures

Technical Specifications

General Properties
Color
The color
White
Evaporation Rate
3.8
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.44

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are provided for product evaluation and are not intended as specification limits.

Property Value Unit Method / condition
NLGI consistency 2 Grade Typical
Color White — Typical
Thickener Fluorinated polymers — Typical formulation
Worked penetration 279 0.1 mm ASTM D217, 60 strokes
Fluorosilicone oil viscosity 2295 SUS At 100°F (38°C)
Specific gravity 1.44 — At 77°F (25°C)
Technical properties

After-processing / final-state properties

Typical in-use and laboratory performance values are provided for product evaluation and are not intended as specification limits.

Property Value Unit Method / condition
Estimated service temperature range -40 to 450 (-40 to 232) °F (°C) Based on formulation and laboratory testing; actual range depends on the application environment
Maximum Dn value 200,000 mm × rpm Estimated; bearing shaft diameter in mm × rotational speed
Bleed 4.5 % CTM0033A, 24 hours at 392°F (200°C)
Evaporation 3.8 % ASTM D2265, 24 hours at 392°F (200°C)
Dropping point >536 (>280) °F (°C) Typical
Water washout <0.3 % ASTM D1264, 1 hour at 175°F (80°C)
4-ball weld load 340 kg ASTM D2596