LORD 410/19GB

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 410/19GB

Main features

  • Glass-Bead Bondline Control
  • 20-30 Minute Working Time
  • Non-Sag Vertical Application

Product Description

LORD 410 / 19GB Acrylic Adhesive System is a two-component structural bonding system combining LORD 410 acrylic adhesive with Accelerator 19GB. The non-sag paste bonds prepared or minimally prepared metals and engineered plastics, including polycarbonate, ABS, acrylics, and XENOY, with a 20 to 30 minute working time at 24 deg C. Accelerator 19GB contains glass beads for controlled bondline thickness, while the mixed system reaches handling strength in 60 to 120 minutes and full cure in 24 hours at room temperature. The service-temperature range is -40 to 149 deg C.

Key features

  • Glass-Bead Bondline Control: Accelerator 19GB contains glass beads for controlled adhesive thickness.
  • 20-30 Minute Working Time: Provides a defined assembly window at 24 deg C.
  • Non-Sag Structural Bonding: Remains in position on vertical and overhead surfaces.

Applications / Suitable for

  • Structural bonding of prepared or minimally prepared metals.
  • Bonding engineered plastics including polycarbonate, ABS, acrylics, and XENOY.
Product Family

LORD 410/19GB

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Off-White to Tan Paste
Density
Volumetric mass per unit
1096 -1156 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
15 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100000 to 300000 mPa.s

Additional Information

Technical properties

Adhesive and accelerator properties

Values apply to LORD 410 adhesive with LORD Accelerator 19GB and are typical unless noted.

Property Value Unit Method / condition
LORD 410 appearance Off-white to tan paste As supplied; typical
LORD 410 viscosity 100,000 to 300,000 mPa s 25 deg C, Brookfield; typical
LORD 410 density 9.15 to 9.65 lb/gal As supplied; typical
LORD 410 flash point 15 deg C Typical
Mix ratio 4:1 by volume LORD 410 adhesive : Accelerator 19GB
Mix ratio 2.91:1 by weight LORD 410 adhesive : Accelerator 19GB
Solids content 100 % Mixed with recommended accelerator; typical
Mixed appearance Tan paste LORD 410 with Accelerator 19GB; typical
Technical properties

Mixed-system and cure properties

Values apply to the LORD 410 / Accelerator 19GB system; cured mechanical data for other accelerator combinations are not included.

Property Value Unit Method / condition
Working time 20 to 30 min 24 deg C; typical
Handling-strength time 60 to 120 min 24 deg C, 60 psi shear criterion; typical
Full-cure time 24 h 24 deg C; typical
Cured appearance Tan to green LORD 410 with Accelerator 19GB; typical
Service-temperature range -40 to 149 deg C Adhesive-system range

Leading Brands Trust in Our Products and Services