LOCTITE TC8M

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE TC8M

Main features

  • High Thermal-Conductivity Silicone Grease
  • Electrical-Insulation Thermal Grease
  • Corrosion-Protective Thermal Grease

Product Description

LOCTITE® TC 8M is a silicone-based thermal grease formulated for efficient heat transfer between heat-generating electronic components and heat-dissipating structures. The material combines high thermal conductivity with excellent electrical insulation and dielectric properties, making it suitable for a broad range of thermal management applications. It retains its paste-like consistency during prolonged exposure to elevated temperatures and is designed for use in semiconductor devices, thermoelectric equipment, radiators, power resistors, and chassis-mounted components. Based on the uploaded datasheet image.

Key Features & Benefits

  • High thermal conductivity for efficient heat dissipation.
  • Excellent electrical insulation properties.
  • High dielectric strength.
  • Maintains paste consistency at elevated temperatures.
  • Suitable for thermal interface applications.
  • Provides corrosion protection on mating surfaces.
  • Easy application using syringes, cartridges, and dispensing equipment.

Recommended Applications

  • Heat sinks in semiconductor devices.
  • Thermostats in thermoelectric devices.
  • Radiators and mounting surfaces.
  • Power resistors.
  • Electronic chassis assemblies.
Product Family

LOCTITE TC8M

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
white
Density (g)
2.5 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1300 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone Grease — Thermal management compound
Appearance White — As supplied
Viscosity 1,300 mPa·s (cP) 25°C, 0.5 rpm
Viscosity 330 mPa·s (cP) 25°C, 5 rpm
Density 2.5 g/cm³ Typical value
Fineness <50 µm Typical value
Shelf Life 365 days 18 to 25°C storage
Operating Temperature Range -40 to +200 °C Continuous operation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Thermal Conductivity 1.5 W/(m·K) Physical property
Weight Loss 0.2 % 24 h @ 100°C
Dielectric Strength 19 kV/mm Electrical property
Volume Resistivity 1 × 10¹⁴ Ω·cm Electrical property
Thermal Management Performance High — Enhances heat transfer between components
Electrical Insulation High — High dielectric and resistivity properties
High Temperature Stability Excellent — Retains paste consistency after heat exposure