LOCTITE SI 5910

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5910

Main features

  • High Movement Flange Sealing
  • Engine Oil Resistance
  • Thixotropic Application Control

Product Description

LOCTITE® SI 5910® is a one-component, room-temperature-vulcanizing oxime silicone sealant supplied as a black thixotropic paste. It is designed for formed-in-place sealing of stamped sheet-metal covers and flanges, including timing covers and oil sumps, where resistance to automotive engine oils and high joint movement is required. The moisture-curing material limits migration after application and develops a flexible elastomeric seal with strong adhesion to metal substrates.

Key features

  • High-movement flange sealing: Produces a flexible cured seal with at least 400% elongation at break.
  • Excellent engine-oil resistance: Supports demanding automotive timing-cover, oil-sump, and flange-sealing applications.
  • Thixotropic one-component application: Requires no mixing and helps reduce migration after dispensing.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.34

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Silicone — Uncured material
Chemical type Oxime silicone — Uncured material
Appearance Black paste — Uncured material
Components One component — No mixing required
Rheology Thixotropic paste — Reduced migration after application
Cure mechanism Room-temperature vulcanizing RTV Atmospheric moisture cure
Specific gravity 1.34 — At 20°C
Extrusion rate 300–650 g/min 0.62 MPa pressure, 15 seconds, 25°C; Semco cartridge
Tack-free time ≤40 min 25°C and 50 ± 5% RH
Density 1.30–1.37 g/cm³ At 25°C; LCT STM 107; SDS value
Flash point >93.3 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on cure time, temperature, humidity, bond gap, substrate, surface preparation, and test method.

Property Value Unit Method / condition
Shore hardness 30 Shore A ISO 868; cured 1 week at 25°C and 50 ± 5% RH
Elongation at break ≥400 % ISO 37; cured 1 week at 25°C and 50 ± 5% RH
Tensile strength ≥1.7 N/mm² ISO 37; cured 1 week at 25°C and 50 ± 5% RH
Tensile strength at 100% elongation 0.6–1.0 N/mm² ISO 37; cured 1 week at 25°C and 50 ± 5% RH
Volume resistivity 1.69 × 1014 Ω·cm IEC 60093; cured material
Surface resistivity 2.81 × 1016 Ω IEC 60093; cured material
Lap-shear strength 0.9–1.4 N/mm² Mild steel; 0.5 mm gap; cured 21 days at 23°C and 60 ± 5% RH
Lap-shear strength 0.6–1.4 N/mm² Aluminum 2024-T3; 0.5 mm gap; cured 21 days at 23°C and 60 ± 5% RH
Lap-shear strength 1.0–1.6 N/mm² Alclad; 0.5 mm gap; cured 21 days at 23°C and 60 ± 5% RH
Lap-shear strength 1.0–1.6 N/mm² Zinc dichromate; 0.5 mm gap; cured 21 days at 23°C and 60 ± 5% RH