LOCTITE SI 5033

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LOCTITE SI 5033

Main features

  • Dual-Cure Sealing Processing
  • Rapid Light Cure
  • Thixotropic Application Control

Product Description

LOCTITE® SI 5033™ is a one-component, dual-cure acetoxy silicone sealant that combines rapid UV/visible light curing with secondary moisture curing for shadowed areas. The non-sag, thixotropic formulation develops functional strength almost instantly upon light exposure and continues to build performance over 72 hours under ambient conditions. Designed for encapsulating, bonding, gasketing, and sealing applications, it forms a high-strength flexible silicone rubber with deep cure capability and excellent environmental resistance.

Key Features & Benefits

  • Dual-cure silicone technology (UV/visible light plus moisture cure).
  • Rapid light cure with deep cure capability.
  • Secondary moisture cure for shadowed areas.
  • Non-sag, thixotropic formulation minimizes migration.
  • Positive UV fluorescence for inspection.
  • Suitable for bonding, encapsulating, sealing and gasketing.
  • Produces a tough, flexible silicone rubber.

Recommended Applications

  • Electronic encapsulation.
  • Gasketing and sealing assemblies.
  • Glass-to-metal bonding.
  • Plastic component bonding.
  • Applications requiring deep UV cure and shadow curing.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light yellow, translucent paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.09

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — Dual-cure UV/moisture system
Chemical Type Acetoxy Dual-Cure Silicone — One-component formulation
Appearance Light Yellow, Translucent Paste — Uncured material
Fluorescence Positive Under UV Light — Inspection aid
Specific Gravity 1.09 — 25°C
Solids Content 95.7 % Non-volatile content
Aspect Ratio (60 sec) 1.0 Height/Width Thixotropic behavior
Extrusion Rate 100 - 170 g/min 0.6 MPa, 25°C
Skin Over Time ≤15 minutes 23°C
Tack-Free Time ≤20 seconds 70 mW/cm² @ 365 nm
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Depth of Cure ≥10 mm 60 sec @ 70 mW/cm², 365 nm
Shore Hardness 45 - 65 Shore A ISO 868
Tensile Strength ≥2.75 N/mm² ISO 37
Elongation at Break ≥150 % ISO 37
Tear Strength 14.0 N/mm ISO 34-1 Die C
Compression Set 4.8 % 22°C, 70 h
Volume Resistivity 1.1 × 10¹⁵ Ω·cm IEC 60093
Dielectric Breakdown Strength 16.2 kV/mm IEC 60243-1
Lap Shear Strength (Glass to Glass) 2.9 N/mm² ISO 4587
Lap Shear Strength (PVC to Glass) 4.1 N/mm² ISO 4587

Leading Brands Trust in Our Products and Services