LOCTITE EA M-121HP

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA M-121HP

Main features

  • Non-Sag Placement Control
  • Two-Part, Room-Temperature-Curing System
  • Prepared Metals Bonding

Product Description

LOCTITE® EA M-121HP™ is a two-part, medium-viscosity, non-sagging epoxy adhesive that cures at room temperature to form a tough, amber-beige bondline. The 2:1 by-volume system combines a 120-minute working life with resistance to peel and impact forces for low-stress structural bonding applications. It bonds prepared aluminum, steel and other metals, as well as selected plastics and ceramics. The cured adhesive also provides documented mechanical and electrical properties, thermal-shock resistance, and resistance to a range of solvents and chemicals.

Key features

  • Toughened, non-sagging epoxy: Forms a tough bondline with documented resistance to peel and impact forces.
  • Extended application window: Provides a typical working life of 120 minutes after mixing.
  • Multi-material bonding: Suitable for bonding prepared metals, selected plastics, ceramics, glass and epoxy-glass materials.

Applications / Suitable for

  • Low-stress structural bonding requiring peel and impact resistance
  • Bonding aluminum, steel, stainless steel and other metals
  • Bonding selected plastics, ceramics, glass and epoxy-glass materials

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two-part
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.07
Physical Properties
Tack-Free Time
140 minutes
Viscosity (Part A)
41,000 to 61,000 mPa.s
Viscosity (Part B)
2,000 to 4,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
90 °C
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
26.5 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed adhesive.

Property Value Unit Method / condition
Components Two components — resin and hardener — As supplied
Appearance Resin: off-white to beige; hardener: amber; mixed: amber-beige — Visual
Mix ratio by volume 2:1 — Resin:hardener
Mix ratio by weight 100:46 — Resin:hardener
Resin viscosity 41,000–61,000 mPa·s (cP) Brookfield RVT, 25°C, spindle 7, 50 rpm
Hardener viscosity 2,000–4,000 mPa·s (cP) Brookfield RVT, 25°C, spindle 5, 50 rpm
Mixed specific gravity 1.07 — 25°C
Working life 120 minutes Typical value after mixing

After-processing / final-state properties

Typical cured-material and adhesive properties. Results depend on the stated cure, substrate preparation and test configuration.

Property Value Unit Method / condition
Glass transition temperature 90 °C ASTM E 228; cured at 25°C except where noted
Tensile strength 40.7 (5,903) N/mm² (psi) ISO 527-2
Elongation 10 % ISO 527-5
Shore hardness 76–90 Shore D ISO 868; cured 16–18 hours at 22°C followed by 2 hours at 65°C
Dielectric breakdown strength 25.6 kV/mm IEC 60243-1
Lap shear strength on grit-blasted steel 29.4 (4,270) N/mm² (psi) ISO 4587; cured 12 hours at 65°C
Lap shear strength on etched and abraded aluminum 33.1 (4,800) N/mm² (psi) ISO 4587; 0.1–0.2 mm gap; cured 12 hours at 65°C