Loctite Ablestik CT 5047-2

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik CT 5047-2

Main features

  • Electrically Conductive Bonding
  • Room Temperature Curing
  • Electrical Connections Bonding

Product Description

LOCTITE ABLESTIK CT 5047-2 is a two-component, electrically conductive epoxy adhesive designed for assembly applications requiring both bonding and electrical connection. The silver-filled system combines a paste resin with an amine hardener at a 100:6 ratio by weight and can be cured at room temperature or with heat. It is intended for electrical connections where hot soldering is impractical and for conductive-plastic locations that cannot be exposed to high temperatures.

Key features

  • Electrically conductive epoxy: Creates bonded electrical connections with typical cured volume resistivity as low as 0.002 ohm-cm after curing for 2 hours at 65°C.
  • Room-temperature or heat cure: Supports a 24-hour cure at 25°C or accelerated cure schedules of 2 hours at 65°C or 1 hour at 100°C.
  • Controlled application window: Provides good dispense behavior and a typical mixed work life of 1 hour for a 100 g mass at 25°C.

Applications / Suitable for

  • Electrical connections where hot soldering is impractical
  • Electrical connection to conductive plastics
  • Assembly locations that cannot be subjected to high temperatures

Technical Specifications

Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.02 Ohms⋅cm
General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
1 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties apply to the separate components or mixed adhesive before cure, as identified.

Property Value Unit Method / condition
Appearance Silver paste — Component A
Appearance Amber liquid — Component B
Mixing ratio 100:6 parts by weight Component A:Component B
Density 3.48 g/cm³ Component A
Density 1.06 g/cm³ Component B
Density 3.34 g/cm³ Mixed adhesive
Work life 1 hour 100 g mixed mass at 25°C
Shelf life 24 months Components A and B at 25°C, from date of manufacture
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule and test conditions.

Property Value Unit Method / condition
Hardness 82 Shore D Cured material
Volume resistivity 0.002 ohm-cm Cured 2 hours at 65°C
Volume resistivity 0.02 ohm-cm Cured 24 hours at 25°C
Tensile lap shear strength 6.9 (1,000) N/mm² (psi) Aluminum-to-aluminum at 25°C
Total mass loss (TML) 0.39 % NASA Reference Publication 1124; sample cured 24 hours at 25°C, plus 2 hours at 65°C, plus 1 hour at 100°C
Collected volatile condensable material (CVCM) 0.0 % NASA Reference Publication 1124; sample cured 24 hours at 25°C, plus 2 hours at 65°C, plus 1 hour at 100°C
Operating temperature -40 to +130 °C TDS reported range