LOCTITE AA H8000

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA H8000

Main features

  • Fast Assembly Fixturing
  • Impact-Resistant Methacrylate Bonding
  • Minimal Surface Preparation Needed

Product Description

LOCTITE® AA H8000™ is a two-component, room-temperature curing methacrylate structural adhesive engineered for rapid bonding of metals, plastics and composite materials. The non-sag adhesive provides fast fixture times, high impact resistance and excellent peel strength while maintaining bond performance across a broad temperature range. Its resilient cured structure and outstanding environmental durability make it suitable for demanding industrial assembly applications involving steel, aluminum, stainless steel, FRP, gelcoat, ABS and other engineering substrates. The product utilizes a 10:1 resin-to-hardener mix ratio and delivers reliable structural performance with minimal surface preparation requirements.

Key Features & Benefits

  • Two-component methacrylate structural adhesive system.
  • Fast fixture time of approximately 25 to 30 minutes.
  • Excellent impact and peel strength performance.
  • Minimal surface preparation required.
  • High elongation and excellent low-temperature impact resistance.
  • Non-sag formulation suitable for vertical applications.
  • Excellent environmental and chemical resistance after cure.
  • Bonds metals, plastics and composites.

Recommended Applications

  • Structural metal bonding assemblies.
  • Composite and FRP fabrication.
  • Plastic-to-metal and plastic-to-plastic bonding.
  • Transportation, industrial equipment and fabricated structures.
  • Applications requiring impact resistance and peel durability.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Yellow/blue
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.97/1.2
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
6,700/6530 mPa.s