LOCTITE AA 3103

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 3103

Main features

  • UV/Visible-Light Adhesive Cure
  • High-Adhesion Adhesive Bonding
  • Polycarbonate Bonding Application

Product Description

LOCTITE® AA 3103™ is a one-component UV and visible light-curing acrylic adhesive specifically formulated for bonding polycarbonate components while minimizing the risk of stress cracking under typical molded stress conditions. The transparent, flexible adhesive cures rapidly upon exposure to suitable ultraviolet or visible light sources, enabling high-speed production processes. LOCTITE AA 3103 develops strong, transparent bonds with a wide variety of substrates including polycarbonate, glass, many plastics and most metals. Its thixotropic consistency reduces adhesive migration after application, allowing precise placement and improved bond-line control.

Key Features & Benefits

  • UV and visible light-curing adhesive for rapid processing.
  • Specially designed for bonding polycarbonate without stress cracking.
  • Forms flexible, transparent bonds.
  • Excellent adhesion to glass, plastics and metals.
  • Thixotropic formulation minimizes adhesive migration.
  • One-component system requiring no mixing.
  • Enhances load-bearing and shock-absorbing characteristics of bonded assemblies.

Recommended Applications

  • Polycarbonate-to-polycarbonate bonding.
  • Transparent plastic assembly applications.
  • Glass-to-plastic bonding.
  • Medical, electronic and industrial component assembly.
  • High-speed production environments utilizing UV curing systems.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent to slightly hazy liquid
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.48
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.13
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
8,000 - 14,500 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — UV / Visible Light Cure
Chemical Type Acrylated Urethane — One-component adhesive
Appearance Transparent to Slightly Hazy — Liquid
Viscosity Classification Medium, Thixotropic — Uncured material
Specific Gravity 1.13 — 25°C
Refractive Index 1.48 — Uncured
Brookfield Viscosity 8,000 - 14,500 mPa·s RVT, spindle 5, 20 rpm, 25°C
Fixture Time ≤18 seconds UV cure, glass microscope slides
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Shore Hardness 51 Shore D ISO 868
Refractive Index 1.50 — Cured adhesive
Elongation at Break 260 % ISO 527-3
Tensile Strength at Break 17 N/mm² ISO 527-3
Tensile Modulus 207 N/mm² ISO 527-3
Lap Shear Strength 11 N/mm² ISO 4587, polycarbonate
Surface Resistivity 8.7 × 10¹⁴ Ω IEC 60093
Volume Resistivity 8.9 × 10¹⁴ Ω·cm IEC 60093
Dielectric Breakdown Strength 24 kV/mm IEC 60243-1