LINQCELL SFP 1000 | Stainless Steel Sintered Fiber Felt

Harmonization Code : 7219141090 | Stainless steel Flat-rolled products of stainless steel, of a width of 600 mm or more

SFP 1000 | Stainless Steel Sintered Fiber Felt

Main features

  • 1mm - 1000um - 39.3mil
  • 304, 304L, 316, 316L, 310s
  • Filter membrane Support

Product Description

LINQCELL SFP1000 is a 1mm Stainless Steel Fiber Felt, meticulously crafted to meet the highest quality standards. This non-woven media is constructed from premium 304, 304L, 316, 316L, 310s stainless steel through a process that randomly lays short stainless steel fibers, followed by sintering and bonding, resulting in an exceptionally durable and efficient material. SFPXXX Series comes in thicknesses ranging from 0.25mm to 1.2mm.

LINQCELL SFP1000 is ideally suited for applications that demand top-tier performance under extreme conditions, such as high pressure, elevated temperatures, and corrosive environments. The fleece of stainless steel fibers can consist of multiple layers, which can be compressed to the desired thickness and then sintered to fuse the individual fibers. The outcome is a highly porous, robust material with remarkable resistance to corrosion, high temperatures, and fractures. Additionally, it offers outstanding permeability, a micron range of 3-100μm and a longer lifespan compared to conventional filtration media.

Key Features:

  • Unlike woven wire mesh, SFP1000 exhibits fine and consistent pore sizes.
  • Easy to work with and mold into various shapes, offering flexibility in application.
  • Excellent for filtration of hot materials and electrical applications due to low electrical heat resistance.
  • Stable Pore Opening: The pore opening remains stable and resists compromise.
  • SFP1000 offers a high dirt holding capacity, ensuring extended service life.
Product Family

LINQCELL SFP1000

1. Select Sheet Size
2. Select Alloy Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Sheet Size and Alloy Type.

Technical Specifications

General Properties
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1000 μm

Additional Information

LINQCELL SFP1000 is an exceptional filtration solution designed to meet the stringent demands of a diverse range of applications. This robust stainless steel fiber felt is engineered to excel in fine, deep, and sub-micron filtration, making it a versatile choice for industries that prioritize efficiency and durability.

Purification of Polymers and Polyester Melt: In the realm of polymer and polyester production, SFP1000 plays a vital role in ensuring the purity and quality of the final products. It effectively removes impurities, resulting in high-grade materials.

Pre-filtration in Ultrafiltration Processes: For ultrafiltration applications, SFP1000 serves as an effective pre-filtration medium, preventing contaminants from clogging or damaging the finer filtration stages.

Filtration in Refining Operations: In refining processes, where the purity of materials is paramount, SFP1000 contributes to the removal of unwanted particles and ensures the quality of the end product.

Electronic Dust Collection for High-Temperature Gases: SFP1000's ability to withstand high temperatures makes it a top choice for electronic dust collection, especially in applications involving hot gases.

Purification of Liquids: Whether it's in the petroleum, food and beverage, biological, or pharmaceutical industries, SFP1000 plays a crucial role in purifying liquids, meeting stringent industry standards.

Protection Filters for Vacuum Pumps: In machinery applications, SFP1000 acts as a protective barrier for vacuum pumps, extending their service life and ensuring efficient operation.

Support for Filter Membranes: SFP1000 provides essential support for filter membranes, enhancing their efficiency and preventing damage from particulates.

Automotive Airbags and Gasbag Aerators: Within the automotive sector, SFP1000 contributes to the reliability of airbag systems and gasbag aerators, ensuring their effectiveness in critical safety applications.

Chemical and Catalyst Recycling: Its fine filtration capabilities are vital in chemical and catalyst recycling processes, minimizing waste and maximizing resource utilization.

Filtering Fuels for Aircraft and Ships: SFP1000 is a trusted choice for fuel filtration, guaranteeing the purity of fuels used in aircraft and ships, where safety is paramount.

Chemical Fiber Filtration: In the production of chemical fibers, SFP1000 assists in maintaining product quality by removing unwanted impurities.

Wastewater Purification: SFP1000 significantly contributes to the purification of wastewater, ensuring that treated water meets environmental standards.

HEPA and ULPA Filters: Its role in HEPA (High-Efficiency Particulate Air) and ULPA (Ultra-Low Penetration Air) filters is essential for achieving high air quality in critical environments.

Materials for Manufacturing Burners: SFP1000 aids in the radiation of materials for burner manufacturing, enhancing the efficiency and performance of these essential devices.

Nuclear Ventilation: In nuclear applications, SFP1000 is a key component of ventilation systems, providing clean and controlled air in sensitive environments.

Viscose Rayon Filtration: Its fine filtration capabilities find applications in viscose rayon production, ensuring the quality and purity of end products.

LINQCELL SFP1000 is a prime example of quality engineering, offering a durable and efficient filtration solution for applications that demand the highest standards of performance, even in the most challenging conditions.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers