LINQCELL GDP250-MP | 250um Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDP250-MP | 250um Carbon Paper

Main features

  • 0.25mm - 250um - 9.85mil
  • Enhanced hydrophobicity from MPL and PTFE coating
  • Optimized as gas diffusion layers in fuel cells

Product Description

LINQCELL GDP250-MP is a 250-µm thick graphitized carbon fiber paper made from high-quality polyacrylonitrile (PAN) fibers. The fibers undergo a wet-laying process to form a non-woven, fibrous, and porous structure, which is then carbonized and graphitized. This high-temperature graphitization (1600 °C) results in high electrical conductivity, high oxidation resistance, and excellent thermal stability, making LINQCELL GDP250-MP highly recommended as gas diffusion layers in fuel cells. It can also be used as gas diffusion substrates for carbon dioxide electrolyzers. 

LINQCELL GDP250-MP has a microporous layer and PTFE coating, which provide hydrophobicity and increased surface area. The higher surface area maximizes catalyst utilization, which increases fuel cell efficiency. Meanwhile, the hydrophobic properties improve water removal and ensure stable operation by preventing flooding within the stack. 

Key Features:

  • 250-µm Thickness: Optimized for reduced stack volume and internal resistance.
  • High-Temperature Graphitization (1600 °C): Provides excellent electrical conductivity, oxidation resistance, and thermal stability.
  • Microporous Layer & PTFE Coating: Enhances hydrophobicity, increases surface area, and optimizes catalyst utilization.
  • Improved Water Management: Hydrophobic properties prevent flooding and ensure stable operation by enhancing water removal.

Highly Recommended As:

LINQCELL GDP250-MP can be customized for specific needs and is available in roll form, with a maximum roll width of 40 cm, providing more flexibility for manufacturing and processing.

Product Family

LINQCELL GDP250-MP

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
99 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
250 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
450 mΩcm
TP Resistance
Opposition to the flow of electric current.
12 mΩcm2
Voltage loss
30 mV