LINQCELL GDL2900 | 2.9mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDL2900 | 2.9mm Carbon Plate

Main features

  • 2.9mm - 2900um - 114mil
  • Thickest GDL available
  • Graphitized Carbon Plate

Product Description

LINQCELL GDL2900 is a graphitized carbon plate, commonly used as a gas diffusion layer and electrode for fuel cells. Its through plane resistance is less than 25 mΩcm2.  It has a thickess of 2.9mm that is measured at 50 kpa.

LINQCELL GDL2900 has a density of ±0.60 g/cm3 and a through plane resistivity of 90mΩ-cm instead of 100mΩ-cm from the classic Spectracarb grades. Voltage loss is 28mV. Shortly, we should be able to die cut circles and most designs that you might require. 

Product Family

LINQCELL GDL2900

1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Sheet Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
1734 g/m2
Density (g)
0.60 g/cm3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
2900 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
87.5 mΩcm
TP Resistance
Opposition to the flow of electric current.
24.5 mΩcm2
Voltage loss
27 mV