LINQCELL GDL1500B | 1.5mm Carbon Plate

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDL1500B | 1.5mm Carbon Plate LINQCELL GDL1500B | 1.5mm Carbon Plate

Main features

  • 1.5mm - 1500um - 59mil
  • Alternative to Spectracarb 6060
  • Improved compressibility

Product Description

LINQCELL GDL1500B is a graphitized carbon plate that boasts impressive technical specifications, making it an excellent choice for use in PEM electrolyzers, PEMFCs, and PAFCs. This carbon paper is commonly used as a gas diffusion layer, porous transport layer and electrode, making it a versatile option for various fuel cell applications.

One of the most notable features of LINQCELL GDL1500B is its low electrical resistance, with a through-plane resistance of less than 21 mΩcm2. This means that it can conduct electricity with high efficiency, making it a reliable and cost-effective choice for fuel cells. Additionally, it has high thermal conductivity, allowing it to transfer heat effectively under high-temperature conditions.

Another key feature of this carbon paper is its high compressibility, which enables it to reach ~1.3mm at 2MPa. This ensures excellent contact with the catalyst layer, promoting optimal performance. Moreover, its durability and low corrosion rate make it a reliable option that can last for extended periods.

LINQCELL GDL1500B is a close alternative to the highly popular and discontinued Spectracarb 6060. This B version retains good strength while having significantly improved compressibility over the original GDL1500 product. It can reach ~1.3mm at 2MPa. It is not only a suitable choice for an electrode or gas diffusion layer, but it also works excellently as a Porous Transport Layer (PTL) in fuel cells. Its high compressibility and porosity allow for optimal reactant transport to the catalyst layer, which is crucial for high-performance fuel cells and electrolyzers.

Applications: PEM Electrolyzers, PEMFCs and PAFCs in distributed power generators

Key Features:

  • High compressibility (>0.3mm at1.5Mpa) 
  • High thermal conductivity 
  • Low electrical resistance
  • Applicable under high temperature
  • High durability and low corrosion

Typically thicker carbon plates such as GDL1500B are specifically suitable for Electrolyzers.

Product Family

LINQCELL GDL1500B

1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Sheet Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
670 g/m2
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1500 μm
Electrical Properties
Through Plane Resistivity
Resistance of the amount of current through a material
140 mΩcm
TP Resistance
Opposition to the flow of electric current.
21 mΩcm2
Voltage loss
39 mV