Main features

  • 1 mil FN polyimide film
  • No adhesive
  • Double Sided FEP

Product Description

LINQTAPE™ PIT1N-FEP616 Series is a general purpose, high-temperature resistant HN polyimide film that is coated on both sides with a 0.1 mil fluorinated ethylene propylene or FEP copolymer.

LINQTAPE™ PIT1N-FEP616 Series is coated with an FEP fluoropolymer coating (F46) emulsified solution and sintered at high temperature to turn general purpose HN polyimide into an FN polyimide. By applying the FEP coating to the HN polyimide film, it is converted to a heat bondable film, which in turn provides a superior moisture barrier and improved chemical resistance.

Product Family

LINQ PIT1N-FEP616

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
None
Chemistry Type
Polyimide
Color
The color
Amber
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
25.4 µm
Special Layer
Double-Sided FEP
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
260 ˚C
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
VOC-Free (100% solids content)
VOC means Volatile Organic compound. VOCs are evaporating molecules and are literally everywhere around us. Our scents are volatile organic compounds, most of the things that we smell are VOC etc. So what do we mean when we state that a product is VOC free? A VOC free product, according to the FTC is one where: 1)VOCs have not been intentionally added to the product. 2)The presence of VOCs at that level does not cause material harm that consumers typically associate with VOCs, including but not limited to, harm to the environment or human health. 3)The presence of VOCs at that level does not result in concentrations higher than would be found at background levels in the ambient air.
Yes

Additional Information

Order Information

Pricing & Availability

Volume Pricing

Volume price breaks are available for each product. Click the specific link under the Description column on the product page to view the live pricing table. Prices are listed without taxes or shipping.

Shipping Hubs

  • EMEA & Africa: Shipped from Amsterdam, Netherlands.
  • Americas: Shipped from Ottawa, Canada.

International Compliance

USA: EIN/TIN required for cross-border shipments.
EU: VAT number required for tax-free intra-community delivery.
Netherlands/Canada: Local taxes apply for domestic addresses.

Payment Options

✔ Credit Card ✔ Bank Transfer ✔ PayPal ✔ Purchase Order*

*Pre-approval required via credit application.

Market Comparison

Competitive Crossovers

Compare LINQTAPE™ price and quality to DuPont, 3M, Nitto, and other leading brands.

Popular Brand Names Product Description KRAYDEN LINQTAPE™ Part#
  • Nitto Permacel P-224
  • DuPont Kapton® Tape
  • 3M 1206
1-mil Single-Sided Polyimide Tape
Acrylic Adhesive
PIT1A-Series
  • Nitto Permacel P-221 / 3M 5413
  • Saint-Gobain Furon® K250
  • Intertape 4428
1-mil Single-Sided Polyimide Tape
Silicone Adhesive
PIT1S-Series
  • Nitto Permacel P-222
  • Saint-Gobain Furon® K350
2-mil Single-Sided Polyimide Tape
Silicone Adhesive
PIT2S-Series
Nitto DuPont 3M Saint-Gobain

Videos & Media

There are no related videos at this time.

Community & Technical Forum

Join the discussion, critique products, and read detailed technical posts on our corporate channels.

Need specialized pricing or assistance?

Contact our support team if you have specific volume requirements or need assistance with international shipping compliance.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers