LAIRD TFLEX 360

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

LAIRD TFLEX 360

Main features

  • 1.50 mm Gap-Filling Solution
  • 50% Deflection at 50 psi
  • 1.2 W/(m K) Thermal Interface

Product Description

Tflex™ 360 is the 1.50 mm-thick configuration of the Tflex™ 300 Series, a ceramic-filled silicone thermal gap filler designed to bridge air gaps between heat-generating components and adjacent heat sinks or enclosures. The light-green thermal interface material provides typical thermal conductivity of 1.2 W/m·K and deflects by more than 50% of its original thickness at 50 psi, enabling effective surface conformity while maintaining reliable thermal contact. Its compliant construction and low compression set make it well suited for electronics requiring a medium-thickness thermal interface.

Key features

  • 1.50 mm thermal gap filler: Specific thickness configuration within the Tflex™ 300 Series for medium-gap thermal interface applications.
  • Highly compliant material: Greater than 50% deflection at 50 psi helps maximize contact across uneven component surfaces.
  • Reliable thermal transfer: Typical thermal conductivity of 1.2 W/m·K with ceramic-filled silicone construction for electronics cooling.

Applications / Suitable for

  • Automotive electronics, ECUs, ADAS, and infotainment systems
  • Networking equipment and telecommunications hardware
  • Industrial electronics and power supplies
  • Consumer electronics requiring compliant thermal gap filling

Technical Specifications

General Properties
Color
The color
Light Green
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Ceramic Filled Silicone Sheet
Density (g)
1.78 g/cm3
Thickness range
1.50 mm
Thermal Properties
Operating Temperature
-40 to 160 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uninstalled properties and available dimensions for the Tflex 300 Series. Values are for design guidance and are not guaranteed specifications. :contentReference[oaicite:1]{index=1}

Property Value Unit Method / condition
Construction and composition Ceramic-filled silicone sheet — Product construction
Color Light green — Visual
Thickness range 1.50 mm Nominal uncompressed thickness range
Density 1.78 g/cc Helium pycnometer
Hardness 51.4 for 20–30 mil
25.2 for 40 mil and above
Shore 00 ASTM D2240; thickness-dependent result
Shelf life 2 years From date of shipment; storage conditions not stated on the product page
Technical properties

After-processing / final-state properties

Typical thermal, electrical, environmental, and installed-interface properties of Tflex 300. Values are not intended as guaranteed design limits. :contentReference[oaicite:2]{index=2}

Property Value Unit Method / condition
Thermal conductivity 1.2 W/m·K ASTM D5470
Thermal resistance 0.98 °C·in²/W Modified ASTM D5470; 40 mil thickness, 10 psi, 50°C
Deflection >50 % At 50 psi; thickness-specific curves are provided in the datasheet
Operating-temperature range -40 to 160 °C Documented product temperature range
Dielectric constant 4.5 — ASTM D150 at 10 GHz
Volume resistivity 1013 ohm·cm ASTM D257
Outgassing TML: 0.56
CVCM: 0.10
wt% ASTM E595
Flammability rating V-0 — UL 94

 