LAIRD CRS-124CRS-124

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD CRS-124CRS-124

Main features

  • Custom Cast Microwave Loads
  • Above-1-GHz RF Attenuation
  • Impact-Resistant Silicone Elastomer

Product Description

Eccosorb CRS-124 Castable Silicone Load Absorber is a two-part, magnetically loaded RTV silicone for forming lossy microwave and RF structures above 1 GHz. The 100:1 Part A-to-Part B weight ratio produces a castable elastomer that can be poured into cavities or molded into cones, wedges, pyramids, terminations, and load shapes. The cured material combines Shore A 75 hardness, 1.0 W/(m K) thermal conductivity, low water absorption, and high volume resistivity. It can also be painted onto surfaces for current suppression or poured in place for microwave gaskets. Applications include microwave loads, RF terminations, cavity filling, antennas, transmission lines, and microwave-tube assemblies.

Key features

  • Castable RF Absorber: Two-part silicone can be poured or molded into custom microwave load geometries.
  • Above-1-GHz Loss Profile: CRS-124 provides high-loss behavior and calculated attenuation data above 1 GHz.
  • Elastomeric Cured Form: Shore A 75 silicone can be shaped to contoured surfaces and withstand impact or shock.

Applications / Suitable for

  • Microwave loads and terminations
  • RF cavity filling and current suppression
  • Microwave gaskets and absorber shapes
  • Antennas and transmission lines
Product Family

LAIRD CRS-124CRS-124

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
<160 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.0 W/m.K
General Properties
Density (g)
4.55 g/cm3
Chemical Properties
Water Absorption
<0.1 %
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
>10^10 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

As-supplied and processing values for the CRS-124 two-part castable system before final cure.

Property Value Unit Method / condition
System format Two-part Part A resin and Part B catalyst
Part A form High-viscosity paste Mix Part A to homogeneity before proportioning
Mix ratio by weight 100:1.00 Part A to Part B for CRS-124
Shelf life approximately 6 months Unmixed in a well-sealed container
Maximum storage temperature 25 deg C Unmixed material
Cure schedule overnight or 3 hours Room temperature overnight or 80 deg C for 3 hours
Technical properties

After-processing / final-state properties

Typical cured CRS-124 properties and theoretical attenuation values for design comparison.

Property Value Unit Method / condition
Frequency range greater than 1 GHz Cured CRS-124
Typical attenuation 20 / 63 / 67 / 149 dB/cm Calculated at 3.0 / 8.6 / 10.0 / 18.0 GHz; comparison only
Service temperature less than 160 deg C Cured material
Thermal conductivity 1.0 W/(m K) Cured material
Hardness 75 Shore A Cured material
Water absorption less than 0.1 % 24-hour test
Dielectric strength greater than 10 V/mil Cured material
Volume resistivity greater than 1 x 10^10 ohm cm Cured material

Leading Brands Trust in Our Products and Services