KESTER 1544

Main features

  • Activated Rosin Oxide Removal
  • Fast Wetting and Capillary Flow
  • Non-Conductive Post-Solder Residue

Product Description

Kester 1544 Activated Rosin Liquid Flux is an alcohol-based, activated rosin flux for electronic soldering, solder coating, and tinning. The ROM1 formulation combines 50% typical solids with rapid wetting and capillary flow where non-activated or mildly activated rosin fluxes do not provide enough oxide removal. It can be applied by brush, dip, or wave methods and supports typical board-side preheat temperatures of 90 to 105 deg C. The post-solder residue is non-conductive and non-corrosive and normally does not require removal. Applications include wave soldering, lead tinning, and assembly processes requiring an activated rosin flux.

Key features

  • Activated Rosin Wetting: ROM1 chemistry supports rapid wetting and capillary flow where stronger oxide removal is required.
  • 50% Solids Flux Control: The high-solids rosin formulation is controlled by specific gravity during use.
  • Non-Conductive Residue: Post-solder residue is non-conductive, non-corrosive, and normally left in place.

Applications / Suitable for

  • Electronic assembly wave soldering
  • Solder coating
  • Tinning bare leads

Technical Specifications

General Properties
Solids
50 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.917–0.928 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-flux properties and storage limits before soldering.

Property Value Unit Method / condition
Flux classification ROM1 J-STD-004
Specific gravity 0.917 to 0.928 At 25 deg C
Typical solids 50 % J-STD-004; IPC-TM-650 Method 2.3.34
Flash point 18 deg C 64 deg F
VOC content 459 g/liter As supplied
Chloride and bromides 0.44 % IPC-TM-650 Method 2.3.35
Shelf life 2 years Stored at 10 to 25 deg C