HUMISEAL 802

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

HUMISEAL 802

Main features

  • UV40 Viscosity Adjustment
  • 2.78 Relative Evaporation Rate
  • 24-Month Shelf Life

Product Description

HumiSeal® Thinner 802 is a proprietary solvent and diluent blend formulated for use with HumiSeal® UV40 conformal coating. It is used to lower the coating’s as-supplied viscosity or restore its original viscosity during processing while maintaining the balance of the compatible coating system. The clear liquid has a relative evaporation rate of 2.78, based on butyl acetate equal to 1, and a specific gravity of 0.86.

Key features

  • UV40 compatibility: Specifically identified for use with HumiSeal® UV40 conformal coating.
  • Viscosity adjustment: Supports lowering the coating’s as-supplied viscosity or restoring viscosity during processing.
  • Balanced solvent blend: Formulated to maintain the original system balance when added to the compatible coating.
  • Clear liquid: Supplied with a specific gravity of 0.86 and a relative evaporation rate of 2.78.

Applications / Suitable for

  • Adjusting the viscosity of HumiSeal® UV40 conformal coating
  • Restoring the original coating viscosity during processing

Technical Specifications

General Properties
Color
The color
clear
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.86
Vapor Density
4
Vapor Pressure
34 mmHg
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
98 °C
Physical Properties
VOC
none

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product type Proprietary solvent and diluent blend — As supplied
Compatible coating HumiSeal® UV40 — Manufacturer-identified compatibility
Color Clear — As supplied
Average weight per gallon 7.17 lb/gal At 20°C
Specific gravity 0.86 — Typical value
Relative evaporation rate 2.78 — Butyl acetate = 1
Boiling point 208 °F Typical value
Vapor pressure 34 mmHg At 68°F
Vapor density 4.0 — Air = 1
VOC None g/L Reported in the supplied TDS
Shelf life 24 months From date of shipment