HUMISEAL 1B73/521

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

HUMISEAL 1B73/521

Main features

  • Ready for Automated Spray Processing
  • 30-Minute Handling Time
  • 50-Cycle -65 to 125 deg C Thermal Shock

Product Description

HumiSeal® 1B73/521 PB25 Acrylic Conformal Coating is a fast-drying, single-component acrylic conformal coating pre-blended to 25 ± 5 cP for automated spray equipment without additional thinning. Intended for printed circuit assemblies, it combines flexibility, UV fluorescence for inspection, and practical repairability with a recommended dry-film thickness of 25–75 µm. Typical handling dry time is 30 minutes, with recommended cure conditions of 24 hours at room temperature or 2 hours at 76°C and seven days to reach optimum properties. The cured coating also has documented thermal-shock, electrical-insulation, dielectric, and fungus-resistance performance.

Key features

  • Ready-to-spray pre-blend: Formulated at 25 ± 5 cP for automated spray equipment without additional thinning.
  • Single-component acrylic coating: Designed for conformal coating of printed circuit assemblies.
  • Fast handling dry: Typical drying time to handle is 30 minutes.
  • UV inspection and repair: Fluoresces under UV light for coating inspection and is easily repaired.
  • Controlled coating thickness: Recommended dry-film thickness is 25–75 µm.
  • Documented cured performance: Includes thermal-shock, dielectric, insulation-resistance, and fungus-resistance data.

Applications / Suitable for

  • Automated spray conformal coating of printed circuit assemblies
  • PCB coating processes requiring UV-assisted inspection
  • Repairable acrylic conformal coating applications
Product Family

HUMISEAL 1B73/521

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Density (g)
0.90 g/cm3
Solids
15 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
42 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
6300 V
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
25 mPa.s

Additional Information

Conformal Coatings | Spray-Ready Acrylic

HumiSeal® 1B73/521 PB25 Acrylic Conformal Coating

HumiSeal 1B73/521 PB25 is a single-component acrylic conformal coating pre-blended for automated spray application without additional thinning. It provides fast handling, UV-fluorescent inspection, repairability, controlled 25–75 µm dry-film application, and documented electrical and thermal performance for printed circuit assemblies.

25 ± 5 cP 15 ± 1 wt% solids 0.90 ± 0.02 g/cm³ 30 min handle 25–75 µm coating UV fluorescent

 

Product data

As-Supplied Properties

Typical exact-product liquid-coating data. Values are representative and are not specifications.

Property Value Unit Method / condition
Product type Single-component acrylic conformal coating — Pre-blended for automated spray application
Density 0.90 ± 0.02 g/cm³ ASTM D1475
Solids content 15 ± 1 % by weight Fed-Std-141, Method 4044
Viscosity 25 ± 5 cP Fed-Std-141, Method 4287
VOC 760 g/L As reported in the exact-product technical data sheet
Shelf life 24 months At room temperature from date of manufacture
Processing

Application and Cure

HumiSeal 1B73/521 PB25 is formulated for automated spray equipment without additional thinning. Successful coating depends on clean, dry assemblies, controlled spray conditions, appropriate ventilation, and compliance with the documented thickness and cure requirements.

Surface cleanliness: Surfaces must be free of moisture, dirt, wax, grease, flux residues, and other contaminants before coating.
Spray application: Use automated spray equipment. The pre-blended formulation is intended for use without additional thinning.
Application environment: Spray at ≤70% relative humidity with adequate ventilation to carry vapor and mist away from the operator.
Thickness and cure: Apply at 25–75 µm dry-film thickness. Typical handling dry time is 30 minutes. Recommended cure is 24 hours at room temperature or 2 hours at 76°C; allow 7 days to reach optimum properties.
Rework: HumiSeal Stripper 1080 is the recommended stripping material.

 

Stage 1
Clean and condition the assembly
Remove moisture and process contaminants, then confirm the coating and assembly have reached the intended application environment.
Stage 2
Apply by automated spray
Spray the pre-blended coating without additional thinning at ≤70% RH, using adequate ventilation and a process targeted to the documented 25–75 µm dry-film range.
Stage 3
Dry, cure and inspect
Plan for 30-minute handling dry, complete the selected cure schedule, and use the coating's UV fluorescence to support coverage inspection before the assembly enters service.
Storage and Handling

Store HumiSeal 1B73/521 PB25 in tightly closed containers away from excessive heat or cold. HumiSeal products may be stored at 0–35°C; before use, allow the coating to equilibrate for 24 hours at 18–32°C. The documented shelf life is 24 months from the date of manufacture at room temperature. The solvent-containing coating is flammable, so application should follow the current Safety Data Sheet and applicable ventilation, ignition-control, personal-protection, storage, and disposal requirements.

Final coating state

Cured Coating Properties

Typical cured-coating data. Preserve the listed test method and condition when comparing or specifying performance.

Thermal shock
50 cycles
MIL-I-46058C, -65°C to 125°C.
Dielectric withstand
>1500 V
MIL-I-46058C.
Insulation resistance
550 TΩ
5.5 × 10¹⁴ Ω per MIL-I-46058C.
Property Value Unit Method / condition
Thermal shock 50 cycles — MIL-I-46058C; -65°C to 125°C
Coefficient of thermal expansion 67 ppm/°C TMA
Glass transition temperature 42 °C DSC
Modulus 11.1 MPa DMA
Dielectric withstand voltage >1500 V MIL-I-46058C
Dielectric breakdown voltage 6300 V ASTM D149
Dielectric constant 2.6 — 1 MHz and 25°C; ASTM D150-98
Dissipation factor 0.01 — 1 MHz and 25°C; ASTM D150-98
Insulation resistance 5.5 × 10¹⁴ Ω MIL-I-46058C; 550 TΩ
Moisture insulation resistance 7.0 × 10¹⁰ Ω MIL-I-46058C; 70 GΩ
Fungus resistance Passes — ASTM G21

RoHS: HumiSeal's Acrylic Conformal Coatings RoHS certificate lists 1B73 preblends as compliant with Directive 2015/863/EU.

Use contexts

Applications

HumiSeal 1B73/521 PB25 is intended for printed circuit assemblies and is specifically formulated for automated spray application. Use should remain within the documented cleanliness, humidity, thickness, cure, inspection, and safety conditions.

Automated PCB conformal coating
Use the 25 cP pre-blend in automated spray equipment when a ready-to-apply acrylic coating is required without an additional thinning step.
UV-assisted coating inspection
The coating fluoresces under UV light, supporting inspection of applied coverage within a controlled conformal coating process.
Repairable coated assemblies
The acrylic coating is easily repaired, with HumiSeal Stripper 1080 identified as the recommended stripping material when removal is required.
Product resource

HumiSeal Acrylic Conformal Coatings RoHS Certificate

The HumiSeal acrylic-coatings certificate identifies 1B73 preblends as compliant with RoHS Directive 2015/863/EU. Use the document to review the listed restricted-substance thresholds and covered acrylic coating families.

Next steps

Technical Support

Work with Krayden to evaluate HumiSeal 1B73/521 PB25 against your automated spray equipment, PCB materials, target dry-film thickness, cure schedule, inspection method, rework requirements, and operating environment. Krayden can help coordinate application trials, process optimization, sampling, and technical support.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers