HumiSeal 1A33LTX Urethane Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal 1A33LTX Urethane Conformal Coating

Main features

  • Fluoresces under UV light for easy inspection and rework
  • Available in pre-blended viscosities for immediate use
  • Easy application using automated coating systems

Product Description

HumiSeal 1A33 LTX is a high-solids, single-component polyurethane conformal coating engineered for maximum reliability in demanding environments. 1A33 LTX provides the best protection of the 1A33 series—offering superior resistance to moisture, dirt, and corrosion—while meeting modern environmental mandates such as GB30981-2020.

Product Key Features

  • Reliable protection against moisture, salt spray, corrosive environments, and dirt
  • Low moisture vapor permeability for long-term electrical reliability
  • Fluoresces under UV light for easy inspection and rework
  • Easy application using automated coating systems
  • Available in pre-blended viscosities for immediate use
  • No free isocyanates
  • Fully compliant with GB30981-2020 VOC requirements

Applications

  • Printed circuit boards (PCBs)
  • Automotive electronics
  • Industrial control systems
  • Consumer electronics
  • Power supplies and converters
  • Electronic assemblies exposed to harsh or corrosive environments
Product Family

HUMISEAL 1A33LTX

1. Select Package Size

Loading pricing…

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
25-75 µm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
26 °C
Operating Temperature
065 - +125 °C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
7500 V

Additional Information

Application Methods

HumiSeal® 1A33 LTX pre-blended products are supplied at controlled viscosities and are ready for immediate use, requiring no additional dilution. Customers should select the appropriate pre-blend based on their coating equipment and application method prior to production use.

Cleanliness of the substrate is critical for successful conformal coating application. PCB surfaces must be free of moisture, dust, wax, grease, flux residues, and other contaminants. Contamination beneath the coating may lead to adhesion failure or reduced long-term reliability.

Application Compatibility

HumiSeal® 1A33 LTX is compatible with automated selective coating systems, spray coating, and dipping processes commonly used in electronics manufacturing. The coating fluoresces under UV light, enabling fast visual inspection, coverage verification, and straightforward repair when required.

Safety and Handling Precautions ⚠️

Application of HumiSeal® conformal coatings must be carried out in accordance with local and national health and safety regulations. The solvents contained in this product are flammable and should not be used near open flames, sparks, or other ignition sources.

Use only in well-ventilated areas to prevent inhalation of vapors or spray mist. Avoid contact with skin and eyes. Always consult the Safety Data Sheet (SDS) before use.

Storage Recommendations 📦

Store HumiSeal® 1A33 LTX and its pre-blended products in tightly closed containers, protected from excessive heat or cold. Recommended storage temperature is between 0°C and 35°C.

Prior to use, allow the product to equilibrate for 24 hours at a room temperature between 18°C and 32°C.

Compliance You Can Trust ✅

  • MIL-I-46058C qualified
  • IPC-CC-830 compliant
  • RoHS Directive 2011/65/EU compliant
  • UL Recognized (File E105698)
  • GB30981-2020 compliant formulation

Leading Brands Trust in Our Products and Services