HARDMAN EPOWELD 58173

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

HARDMAN EPOWELD 58173

Main features

  • 5-Minute Gel Time
  • Cure Down to -18 deg C
  • Multi-Substrate Epoxy Bonding

Product Description

EPOWELD® 48173/58173 is an extra fast setting, two-component, room temperature curing epoxy adhesive designed to bond metal, wood, concrete, ceramics, and many plastics. It is highly effective for fast patching, fixturing, and repairs requiring quick handling strength, with the unique ability to cure at temperatures as low as -18°C (0°F).

Key features

  • Fast setting and gel time: Offers a quick 5-minute gel time and rapid handling strength for efficient repair and fixturing workflows.
  • Low temperature cure: Capable of curing at extreme temperatures as low as -18°C (0°F), allowing for versatile application environments.
  • Convenient mix ratio: Features a user-friendly 1:1 mix ratio by volume, simplifying dispensing and application.

Applications / Suitable for

  • Bonding metal, wood, concrete, ceramics, and many plastics.
  • Fast patching and fixturing applications.
  • General repairs requiring quick handling strength.

Technical Specifications

General Properties
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5 minutes (Gel time) minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure physical and processing characteristics of mixed EPOWELD® 48173/58173.

Property Value Unit Method / condition
Appearance / Color (Mixed) Amber - -
Mix Ratio (Volume) 1:1 (100:100) - Part A to Part B
Mix Ratio (Weight) 100:94 - Part A to Part B
Viscosity (Mixed) 40,000 cps at 25°C
Specific Gravity (Mixed) 1.16 - at 25°C
Gel Time 5 minutes 4 gm mass at 25°C
Technical properties

After-processing / final-state properties

Typical cured mechanical properties of EPOWELD® 48173/58173 when tested at 25°C.

Property Value Unit Method / condition
Hardness 80 Shore D Tested at 25°C
Lap Shear Strength 3,000 psi Acid-etched Al/Al, cured 24 hrs @ 25°C, tested at 25°C
T-Peel Strength 1.8 pli Acid-etched Al/Al, cured 24 hrs @ 25°C, tested at 25°C

Leading Brands Trust in Our Products and Services