FREKOTE R-150

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

FREKOTE AQUALINE R-150

Main features

  • Non-Flammable Mold Release Formulation
  • Natural/Synthetic Rubber Release and Slip
  • 60 to 200 deg C Mold Operation

Product Description

LOCTITE® FREKOTE® R-150™, formerly known as AQUALINE® R-150™, is a water-based, heat-curing mold release agent for demanding rubber molding processes, particularly those involving highly abrasive compounds. Applied as a finely atomized spray to a preheated mold, it chemically bonds to the surface and forms a thin, inert, thermally stable release coating. The product supports the release of natural and synthetic rubber compounds, thermoplastic urethanes, and certain solid polyurethane cast elastomers while providing release and slip performance across mold application temperatures from 60 to 200°C.

Key features

  • Water-based formulation: Supplied as a non-flammable, translucent emulsion with mild odor.
  • Release and slip performance: Recommended for demanding rubber molding applications, including highly abrasive compounds.
  • Heat-curing release coating: Forms a thin, inert coating on preheated molds and supports multiple releases.
  • Broad mold-temperature window: Applied to molds operating from 60 to 200°C.
  • Freeze/thaw stable: Supports storage and handling where temperature cycling may occur.

Applications / Suitable for

  • Natural and synthetic rubber molding compounds
  • Highly abrasive rubber compounds
  • Thermoplastic urethanes
  • Certain solid polyurethane cast elastomers
Product Family

FREKOTE R-150

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Translucent emulsion
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.98–1.02
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
315 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics of LOCTITE® FREKOTE® R-150™.

Property Value Unit Method / condition
Appearance Translucent emulsion — As supplied; LMS-controlled characteristic
Chemical type Water-based emulsion — As supplied
Odor Mild — As supplied
Specific gravity 0.98–1.02 — At 25°C; LMS-controlled characteristic
pH 3.9–4.1 — LMS-controlled characteristic
Cure mechanism Heat cure — Applied to a preheated mold
Technical properties

After-processing / final-state properties

Documented characteristics of the heat-cured release coating.

Property Value Unit Method / condition
Cured thermal stability ≤315 °C Heat-cured release coating
Release-film form Thin, inert coating — Formed after application to a preheated mold and heat curing