EUREMELT 3413

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

EUREMELT 3413

Main features

  • 2.8 to 4.0 Pa s Melt Viscosity
  • Flexibility to -35 deg C
  • 23 kV/mm Dielectric Strength

Product Description

EUREMELT 3413 is a black copolyamide thermoplastic hot-melt adhesive supplied as granules for low-pressure injection molding around electrical and electronic devices. It combines a specified softening point of 150–160 °C with a specified melt-viscosity range of 2.8–4.0 Pa·s at 210 °C. The material is applied at 180–220 °C and provides flexible molded encapsulation, including low-temperature flexibility to −35 °C. It adheres to PVC and other plastics and is used where low-pressure molding must form a protective molded body around components, connectors, wiring, or related assemblies. Typical electrical properties include 23 kV/mm dielectric strength, 3 × 1012 Ω·cm specific resistance, and CTI 600.

Key features

  • Low-pressure molding grade: Thermoplastic copolyamide hot melt for casting electrical devices by low-pressure injection molding.
  • Controlled melt processing: Specified melt viscosity of 2.8–4.0 Pa·s at 210 °C and an application-temperature range of 180–220 °C.
  • Low-temperature flexibility: Typical flexibility to −35 °C according to ASTM D 3111.
  • Electrical insulation data: Typical dielectric strength of 23 kV/mm, specific resistance of 3 × 1012 Ω·cm, and CTI 600.
  • Plastic adhesion: Documented adhesion to PVC and other plastics.

Applications / Suitable for

  • Low-pressure molding and encapsulation of electrical devices
  • Connectors, cable assemblies, and wire-harness components
  • Printed circuit assemblies, sensors, coils, relays, and related electronic components
Product Family

EUREMELT 3413

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
23 kV/mm

Additional Information

Hot-melt adhesive for low-pressure molding

EUREMELT 3413

EUREMELT 3413 Black is a granulated copolyamide thermoplastic hot melt for low-pressure injection molding around electrical and electronic devices. Its controlled melt viscosity, flexible molded state, plastic adhesion, and electrical insulation data support evaluation for connectors, wiring assemblies, sensors, and related encapsulated components.

Copolyamide hot melt Black granulate 150–160 °C softening point Flexible to −35 °C
EUREMELT 3413 Black granulated hot-melt adhesive in its approved product packaging

EUREMELT 3413 Black is supplied as black granules for melt processing.

Material data

As-supplied and melt properties

Specified values are guaranteed key data. Other listed values are typical and provided for product evaluation.

Property Value Unit Method / condition
As-supplied form Granulate — Black
Amine value ≤ 3 mg KOH/g ISO 9702; specified
Acid value ≤ 10 mg KOH/g ISO 2114; specified
Softening point R+B 150–160 °C ISO 4625; specified
Melt viscosity 2.8–4.0 Pa·s ISO 2884 at 210 °C; specified
Melt viscosity 4 Pa·s ISO 2884 at 200 °C; typical
Low-pressure molding process

Melt, inject, cool, and demold

The granulated material is thermally melted and injected around the electrical or electronic assembly using a low-pressure molding process. EUREMELT 3413 does not require reactive mixing or chemical cure; the molded part develops through cooling after injection.

Application temperature: 180–220 °C.
Open time on paper: 6–10 seconds at 23 °C after application at 200 °C; typical.
Open time, canal method: 20–28 seconds at 23 °C after application at 200 °C; typical.
Setting time: 1–3 seconds on Nora test rubber at 23 °C after application at 200 °C; typical.
Illustrative low-pressure molding sequence showing granules melted, injected around an electrical assembly, cooled, and demolded

Insert an approved process visual showing the low-pressure molding sequence for an electrical assembly.

Storage and handling

Store EUREMELT 3413 Black in a dry place, preferably in the sealed original packaging, between 2 and 40 °C and away from direct sunlight. The stated shelf life is two years; refer to the expiry date on the original container.

Molded material data

Final material properties

Values in this section are typical unless otherwise indicated. They are not guaranteed design specifications.

Property Value Unit Method / condition
Shore hardness 86 A / 28 D Shore DIN ISO 7619 at 23 °C
Low-temperature flexibility −35 °C ASTM D 3111
Tensile strength ≥ 4 N/mm² DIN EN ISO 527 at 23 °C
Elongation at tensile strength ≥ 250 % DIN EN ISO 527 at 23 °C
Dielectric constant 3.5 — 1 MHz
Specific resistance 3 × 1012 Ω·cm 24 °C
Dielectric strength 23 kV/mm Typical
Tracking resistance CTI 600 — Test solution A
Water absorption 0.7 / 1.5 / 2.35 / 2.75 % DIN EN ISO 62 at 23 °C after 24 h / 4 d / 14 d / 28 d
Use contexts

Low-pressure molding applications

EUREMELT 3413 is positioned as a standard, broadly applicable grade for low-pressure molding. Final suitability depends on the component design, materials, molding conditions, and end-use requirements.

Low-pressure molded printed circuit assembly or sensor protected within a thermoplastic polyamide body
Printed circuit assemblies and sensors
The low-pressure molding process can surround delicate electronic assemblies without a reactive cure step. The grade’s controlled melt viscosity and electrical insulation data are relevant when evaluating molded protection around boards, sensors, or related components.
Electrical connector or wire harness overmolded with black low-pressure molding material
Connectors and wire harnesses
EUREMELT materials are used in low-pressure molding of automotive and industrial connectors, cable bundles, and electrical wire harnesses. EUREMELT 3413 provides a black flexible molded body and documented adhesion to PVC and other plastics.
Coil, relay, transformer, or microswitch encapsulated by low-pressure thermoplastic molding
Coils, relays, and compact electrical devices
The product family is used for coils, relays, microswitches, transformers, and other electrical devices. The 3413 grade’s flexibility, fast-setting thermoplastic behavior, and insulation properties support evaluation for these molded component formats.
Next steps

Evaluate EUREMELT 3413 for your molding process

Contact Krayden to discuss component materials, mold design, processing temperature, melt-flow requirements, electrical-property needs, samples, or grade selection for a low-pressure molding application.