Main features

  • Low Melt Viscosity
  • Rapid One-to-Three-Second Setting
  • Plastics and Porous Substrates

Product Description

EUREMELT 2888 Polyamide Hot Melt Adhesive is an amber polyamide thermoplastic hot melt adhesive supplied in pellet form for bonding plastics and porous substrates. stated substrate uses include PVC, ABS, polycarbonate, wood, and leather, with a filter-bonding context also identified. The adhesive has a softening point of 185 to 190 deg C and an application temperature range of 200 to 230 deg C. Typical melt viscosity is 4,000 to 6,000 cP at 220 deg C, and the setting time is 1 to 3 seconds under the stated test condition.

Key features

  • Low melt viscosity: Typical viscosity is 4,000 to 6,000 cP at 220 deg C.
  • One-to-three-second setting: The adhesive develops a rapid set under the documented test condition.
  • Plastics and porous substrates: Supported bonding uses include PVC, ABS, polycarbonate, wood, and leather.

Applications

  • Bonding PVC, ABS, and polycarbonate
  • Bonding wood and leather
  • Filter-bonding applications
Product Family

EUREMELT 2888

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber Pellets
Other Properties
Storage Temperature
2 - 40 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pellet, melt-processing, open-time, setting, hardness, and storage data.

Property Value Unit Method / condition
Form as supplied Amber pellets - Visual
Softening point 185 to 190 deg C ISO 4625, ring-and-ball
Melt viscosity at 220 deg C 4,000 to 6,000 cP ISO 2884
Melt viscosity at 200 deg C 2,100 cP ISO 2884
Application temperature 200 to 230 deg C Recommended processing range
Open time on silicon paper 11 to 15 s At 23 deg C; adhesive applied at 220 deg C
Open time, canal method 25 to 31 s At 23 deg C; adhesive applied at 220 deg C
Setting time 1 to 3 s Nora test rubber at 23 deg C; applied at 220 deg C
Hardness 96A / 50D Shore DIN ISO 7619 at 23 deg C
Shelf life 2 years Dry original packaging at 2 to 40 deg C