EPOCAST 1614-A3 Epoxy Structural Syntactic Adhesive is a low-density, flame-retardant, one-component frozen epoxy structural syntactic adhesive for aerospace honeycomb composite reinforcement and bonding. The premixed paste provides up to 16 hours of working life and typical wet density below 0.75 g/cm^3. It cures at elevated temperature and retains typical compressive strength of 7.0 to 9.0 ksi at 177 deg C after the stated cure. Applications include honeycomb core reinforcement, structural joining, fastener or attachment potting, and panel-edge reinforcement.

Key features

  • Premixed frozen format: The one-component paste is supplied premixed and frozen for controlled preparation before use.
  • Extended working life: Working life is up to 16 hours, depending on process requirements.
  • Elevated-temperature strength: Typical compressive strength is 7.0 to 9.0 ksi at 177 deg C after cure.

Applications

  • Honeycomb core reinforcement
  • Structural bonding and joining
  • Fastener or attachment potting
  • Panel-edge reinforcement

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
reddish brown paste
Density (g)
0.7-0.75 g/cm3
Physical Properties
Extrusion Rate
> 1000 g/min
Other Properties
Storage Temperature
-18 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values apply to the frozen one-component material before cure.

Property Value Unit Method / condition
Appearance Reddish brown paste - Visual
Wet density < 0.75 g/cm^3 ASTM D1875
Viscosity Paste - ASTM D2196 at 25 deg C
Extrusion rate > 1,000 g/min At 25 deg C after 8 hours; OEM method
Sag resistance <= 0.1 in OEM method
Working life Up to 16 h Depends on process requirements
Shelf life 6 months Stored at -18 deg C or lower in the original sealed container
Technical properties

After-processing / final-state properties

Typical cured values remain paired with the stated cure and test temperatures.

Property Value Unit Method / condition
Cure cycle 90 at 127 deg C; 60 at 177 deg C min Material temperature; typical 2 to 4 deg C/min ramp
Cured density 0.70 to 0.75 g/cm^3 ASTM D1622
Compressive strength at 23 deg C 13 to 16 ksi ASTM D695
Compressive strength at 149 deg C 8.0 to 10.0 ksi ASTM D695
Compressive strength at 177 deg C 7.0 to 9.0 ksi ASTM D695
Tensile lap shear 1.2 to 1.5 ksi Aluminum-to-aluminum at 23 deg C; ASTM D1002
Glass transition temperature 372 (190) deg F (deg C) TMA; ASTM E1824; cured 1 hour at 177 deg C
CTE below Tg 34 um/(m deg C) ASTM E831; cured 1 hour at 177 deg C