EPIBOND 1217

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPIBOND 1217

Main features

  • Quick-Set Epoxy Adhesive
  • Room-Temperature Epoxy Cure
  • 1:1 Mix Ratio

Product Description

Epibond® 1217 A/B Epoxy Adhesive is a two-part, translucent epoxy adhesive system designed for rapid bonding of steel, aluminum, wood, ceramics, and a variety of polymeric substrates. This room-temperature-curing adhesive uses a simple 1:1 mix ratio by weight or volume and develops handling strength quickly, making it suitable for fast assembly and repair operations. The material is supplied as a paste and is available in twin-cartridge packaging for dispensing through static mixing equipment. Typical cured lap shear strength on aluminum reaches 2,500 psi (17.2 MPa) at 25°C, providing strong adhesion across a range of common engineering materials.

Key features

  • Fast room-temperature cure: Typical cure is achieved within 1 to 2 hours at 25°C for rapid assembly processes.
  • Simple 1:1 mix ratio: Equal-volume and equal-weight mixing simplifies dispensing and processing.
  • Strong structural bonding: Typical aluminum-to-aluminum lap shear strength reaches 2,500 psi (17.2 MPa) at 25°C.

Applications / Suitable for

  • Bonding steel components
  • Bonding aluminum assemblies
  • Wood bonding applications
  • Ceramic assembly and repair
  • Bonding a variety of polymeric substrates

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent
Density (g)
1.19 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing and material properties for the supplied resin, hardener, and mixed adhesive system.

Property Value Unit Method / condition
Mix ratio 1:1 Volume / Weight Part A : Part B
Density (mixed) 1.19 g/cm³ ASTM D792, 25°C
Gel time 4-8 minutes 50 g sample at 25°C
Appearance Translucent - Mixed system, visual
Typical cure cycle 1-2 hours 25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive performance values measured on aluminum test specimens.

Property Value Unit Method / condition
Tensile lap shear 2,500 (17.2) psi (MPa) ASTM D1002, Al-Al, 25°C
Tensile lap shear 1,350 (9.3) psi (MPa) ASTM D1002, Al-Al, -55°C
Tensile lap shear 500 (3.4) psi (MPa) ASTM D1002, Al-Al, 83°C