ELANTAS K-230

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ELANTAS K-230

Main features

  • 100% Solids Epoxy Processing
  • Room-Temperature Cure Route
  • Bonding Across Thermal Expansion Differences

Product Description

EASYPOXY K-230 Two-Component Epoxy Adhesive is a 100% solids, room-temperature-curing epoxy adhesive and repair compound. The two-component system supports general-purpose bonding and repair, including assemblies that join materials with different coefficients of expansion. Its ambient cure route permits bonding without a required production oven, while the 100% solids formulation defines the supplied resin system. K-230 is suited to repair operations and bonded assemblies where dissimilar thermal expansion is an important material-selection factor and a two-part epoxy process is acceptable.

Key features

  • 100% Solids Formulation: The adhesive is supplied as a two-component 100% solids epoxy system.
  • Room-Temperature Cure: The material develops its bond through an ambient cure route.
  • Dissimilar-Expansion Bonding: Applications include joining materials with different coefficients of expansion.

Applications / Suitable for

  • General-purpose bonding
  • Adhesive repair work
  • Bonding materials with different coefficients of expansion

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Chemical Properties
Water Absorption
0.4 %
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
4.0 x 10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the individual components before mixing and curing.

Property Value Unit Method / condition
Viscosity 100,000 / 50,000 cP Part A Resin / Part B Hardener @ 25°C
Specific Gravity 1.17 / 1.08 — Part A Resin / Part B Hardener @ 25°C
Mix Ratio 100 : 45 By weight Part A : Part B
Work Life 60 minutes 25°C / 77°F
VOC Content <0.1 % ASTM D6053
Technical properties

After-processing / final-state properties

Typical cured properties of EASYPOXY® K-230.

Property Value Unit Method / condition
Shore Hardness D80 — ASTM D2240, 25°C
Lap Shear Strength 2,500 psi ASTM D1002, etched aluminum/aluminum, 25°C
Compressive Strength 18,000 psi ASTM D695, 25°C
Flexural Strength 10,000 psi ASTM D790, 25°C
Volume Resistivity 4.0 × 10¹³ ohm-cm ASTM D257, 25°C
Thermal Conductivity 0.2 W/m·K 25°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers