DYMAX 9-911

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DYMAX 9-911

Main features

  • Multi-cure technology
  • High viscosity gel
  • Blue, fluorescent inspection

Product Description

Dymax Multi-Cure® 9-911-REV-B is a light-curable, wire-tacking adhesive formulated for rapid attachment of repair and jumper wires on printed circuit boards. This acrylated urethane adhesive cures with UV and visible light and includes a secondary heat-cure capability for shadowed areas where light exposure is limited. Its high-viscosity gel consistency helps maintain wire placement and board coverage during assembly and repair operations. The material provides strong adhesion to circuit board components, resists solvents after cure, and is supplied as a one-part system that requires no mixing. The adhesive is also RoHS compliant and fluoresces blue for process inspection and verification.

Key features

  • Multi-cure technology: UV/visible light curing with secondary heat-cure capability supports curing in shadowed or light-obstructed areas.
  • High-viscosity gel: Nominal viscosity of 25,000 cP helps maintain wire positioning and coverage during PCB repair and assembly.
  • Blue fluorescent inspection: Fluoresces under appropriate inspection conditions to support bond-line verification and quality control.

Applications / Suitable for

  • Wire tacking on printed circuit boards
  • Bonding jumper wires
  • PCB repair operations
  • Electronic assembly applications requiring rapid fixture times
Technical properties

As-supplied / before-processing properties

Typical as-supplied properties of Dymax Multi-Cure® 9-911-REV-B prior to curing.

Property Value Unit Method / condition
Chemical Class Acrylated Urethane N/A Material type
Appearance Clear Translucent Gel N/A Visual
Density 1.07 g/mL ASTM D1875
Viscosity 25,000 (nominal) cP 20 rpm, DSTM 502
Shelf Life 7 months Stored at 10°C to 35°C in unopened container

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless Translucent Gel
Chemistry Type
Acrylated Urethane
Density (g)
1.07 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
25,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 %
Chemical Properties
Water Absorption
1.3 %
Other Properties
Storage Temperature
10 - 32 °C