DOWSIL SE 9189 L

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL SE 9189 L

Main features

  • One-Part Flowable RTV Silicone Adhesive
  • Eight-Minute Tack-Free Time
  • 25 kV/mm Dielectric Strength

Product Description

DOWSIL SE 9189 L RTV Adhesive is a one-part gray or white moisture-cure silicone with flowable rheology for electronics assembly. Typical viscosity is 22,000 cP and tack-free time is 8 minutes at 25 deg C before the material cures to a soft elastomer with documented mechanical and dielectric properties. The product supports needle dispensing and flow application and is used for circuit-board component fixing, vibration dampening, and sealing.

Key features

  • Flow and dispensing: One-part flowable RTV silicone with typical 22,000 cP viscosity for needle dispensing or flow application.
  • Processing window: Typical tack-free time is 8 minutes at 25 deg C under the documented moisture-cure process.
  • Electrical performance: Typical cured properties include Shore A 33 hardness, 220% elongation, 2.0 MPa tensile strength, and 25 kV/mm dielectric strength.

Applications

  • Circuit-board component fixing
  • Vibration dampening
  • Sealing

Technical Specifications

General Properties
Color
The color
White or Gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.19
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
22000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
220 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
25 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
9E14 Ohms⋅cm

Additional Information

Electronics Assembly Adhesives

Flowable one-part RTV silicone for fixing, damping, and sealing

DOWSIL SE 9189 L RTV Adhesive is a one-part gray or white moisture-cure silicone with flowable rheology for electronics assembly. The product has a typical viscosity of 22,000 cP and 8-minute tack-free time at 25 deg C, then cures to a soft elastomer with documented mechanical and dielectric properties.

1-part moisture cure22,000 cP viscosity8 min tack-freeShore A 3325 kV/mm dielectric strength

As-Supplied Properties

Flowable one-part silicone before cure

The material is supplied as a single-component gray or white silicone with a typical viscosity of 22,000 cP and flowable application behavior.

Property Typical Value Unit / Condition State
Component count One - As supplied
Color Gray or white - As supplied
Viscosity 22,000 cP As supplied
Low molecular weight siloxane, D4-D10 20 ppm As supplied / product value
Low molecular weight siloxane, D4-D20 110 ppm As supplied / product value

Processing

Dispense or flow onto prepared surfaces and allow moisture cure

SE 9189 L supports needle dispensing and flow application. Surface preparation and access to atmospheric moisture remain important to adhesion and through-cure.

  1. Clean the surfaces:Thoroughly clean or degrease bonding surfaces using a suitable method for the actual substrate. Residual oils can interfere with adhesion.
  2. Apply the material:Use automated or manual needle dispensing, or a flow application method, according to the required fixing, damping, or sealing geometry.
  3. Allow surface cure:Typical tack-free time is 8 minutes at 25 deg C. Cure progresses from the exposed surface inward because the one-part system relies on moisture in the air.
  4. Accelerate when appropriate:Mild heat below 60 deg C can accelerate the moisture-cure process when appropriate.

Storage & Handling

Exclude moisture before use

Store at or below the temperature shown on the product label, keep the original container tightly closed, and minimize headspace. For partially filled containers, purge with dry air or another dry gas such as nitrogen and use the product by the label Use Before date.

Technical Guidance

Control substrate condition, cure depth, and service exposure

The product is flowable, but final bond or seal performance still depends on the actual substrate, joint geometry, and moisture-cure environment.

Test the actual substrate

Test the actual substrate because surface chemistry and contamination can change adhesion. A lap-shear or similar test can be used to evaluate compatibility and minimum cure time.

Avoid unsupported deep-section assumptions

One-part moisture-cure silicones cure from the exposed surface inward and are not typically used in highly confined spaces or where deep-section cure is required.

Keep solvent exposure intermittent

The supplied guidance is for splash or intermittent solvent exposure rather than continuous solvent or fuel exposure. Confirm the actual fluid and exposure condition before use.

Final-State Properties

Typical cured and bonded performance

The table reports cured mechanical and electrical properties and preserves the documented bonded glass test configuration where applicable.

Property Typical Value Unit / Test Condition State
Specific gravity 1.19 Cured Cured material
Lap shear adhesion 120 N/cm2 on glass Bonded test
Tensile strength 2.0 MPa Cured material
Elongation 220 % Cured material
Durometer 33 Shore A Cured material
Dielectric strength 25 kV/mm Cured material
Volume resistivity 9.0 E+14 ohm-cm Cured material
Dielectric constant 3.1 at 1 MHz Cured material
Dissipation factor 0.0004 at 1 MHz Cured material

Applications

Documented electronics assembly uses

SE 9189 L is positioned for fixing, vibration management, and sealing functions on electronic assemblies.

Circuit-board component fixing

Flowable RTV adhesive for fixing parts on circuit boards where a soft cured silicone is appropriate.

Vibration dampening

Application around supported electronic parts to provide a soft elastomeric material for vibration-dampening use.

Sealing

Flowable silicone sealing around supported electronics interfaces and assemblies.

Technical support for DOWSIL SE 9189 L RTV Adhesive

Need help evaluating SE 9189 L for component fixing, vibration dampening, or a sealing joint? Krayden can help review substrate preparation, dispense or flow application, section geometry, moisture-cure conditions, and the mechanical or dielectric properties required by the intended electronics assembly.

Contact Us

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers