DOWSIL DS-2025

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL DS-2025

Main features

  • Cured Silicone Residue Removal
  • Up to 400 g/L Silicone Solubilization
  • Below 10 cP Low Viscosity

Product Description

DOWSIL™ DS-2025 Silicone Cleaning Solvent is a low-viscosity, hydrocarbon-based cleaning solvent containing a catalytic depolymerization agent. It removes cured and uncured silicone residues from contaminated surfaces, tools, process equipment, tanks, and manufacturing units by digesting and dissolving silicone deposits. The liquid works without water and is intended for direct, continuous contact through equipment immersion, tank filling, or recirculation. It has a closed-cup flash point above 90°C and can solubilize up to 400 g of silicone per liter, allowing multiple cleaning uses before saturation. A follow-up degreasing step with DOWSIL™ DS-1000 Aqueous Silicone Cleaner is recommended after the used solvent is drained and collected.

Key features

  • Catalytic silicone removal: Depolymerizes and dissolves substantive cured silicone deposits to leave a silicone-free surface.
  • Low-viscosity liquid: Viscosity below 10 cPs at 20°C supports direct contact through immersion, tank filling, or recirculation.
  • Multiple-use cleaning capacity: Can solubilize up to 400 g of silicone per liter before becoming saturated.

Applications / Suitable for

  • Removing cured or uncured silicone residues from surfaces and tools
  • Cleaning process equipment and meter/mix equipment components
  • Cleaning tanks and manufacturing units contaminated with cured silicone deposits

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light brown liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.85
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
20 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance Light brown liquid — Typical
Odor Slight solvent odor — Typical
Specific gravity 0.85 — CTM 1100G
Viscosity < 10 cPs ISO 104/3105; 20°C
Flash point > 90 °C ASTM D93; closed-cup method
Usable life 60 months From date of production when stored in a cool, dry place in the original unopened container

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers