DOWSIL 9-1363

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 9-1363

Main features

  • Fast Skin-Over and Tack-Free Development
  • Primerless Multi-Substrate Adhesion
  • Neutral-Cure Silicone Adhesive

Product Description

DOWSIL™ 9-1363 Industrial Assembly Adhesive Sealant is a one-part, 100% silicone RTV adhesive sealant for original equipment manufacturer assembly applications. The neutral-cure material combines sealing and bonding functions with fast surface-cure characteristics that allow assembled parts to be handled more quickly than with traditional RTV sealants. It is supplied as a paste and provides good unprimed adhesion to many substrates. The neutral cure chemistry produces a non-vinegar odor and will not corrode brass or copper, supporting evaluation for assemblies containing these metals. The material requires atmospheric moisture to cure and should not be used in totally confined spaces.

Key features

  • Fast surface cure: A skin-over time of 1–2 minutes and tack-free time of 5–10 minutes support quick handling during OEM assembly.
  • Unprimed adhesion: Provides good adhesion to many substrates without a primer in most applications.
  • Neutral-cure silicone: Produces a non-vinegar odor and will not corrode brass or copper.

Applications / Suitable for

  • Assembly sealing in original equipment manufacturer applications
  • Adhesive bonding of parts in OEM assemblies
Product Family

DOWSIL 9-1363

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray, white, black paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.34
Physical Properties
Tack-Free Time
5–10 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
350 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the material as supplied. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Available colors Gray, white, black — As supplied
Consistency Paste — As supplied
Slump 0.2 inch Test method not stated
Extrusion rate 200 grams/minute CTM 0364; 1/8-inch nozzle at 90 psi
Skin-over time 1–2 minutes Test method not stated
Tack-free time 5–10 minutes CTM 0095
Specific gravity 1.34 — CTM 0097
Cure-in-depth time 24 hours 1/8-inch depth at 23°C (73°F) and 50% RH

After-processing / final-state properties

Typical cured-material properties after seven days at 25°C (77°F) and 50% relative humidity. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Durometer hardness 33 Shore A points CTM 0099; after 7 days at 25°C (77°F) and 50% RH
Tensile strength 240 psi CTM 0137A; after 7 days at 25°C (77°F) and 50% RH
Elongation 350 % CTM 0137A; after 7 days at 25°C (77°F) and 50% RH
Modulus at 100% elongation 120 psi After 7 days at 25°C (77°F) and 50% RH; test method not stated