CYBERBOND 2999

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2999

Main features

  • Surface-Insensitive Porous-Material Bonding
  • Thixotropic Vertical-Surface Control
  • High-Viscosity Gap Filling

Product Description

Cyberbond CB 2999 is a one-part, surface-insensitive ethyl cyanoacrylate gel for fast bonding on acidic and porous materials as well as common engineering substrates. Its thixotropic, very high-viscosity profile keeps the adhesive in place on vertical surfaces and supports gap filling without the flow behavior of lower-viscosity grades. The colorless, transparent adhesive has cone-and-plate viscosity of 35,000 to 60,000 cP at 0.5 rpm and 3,000 to 6,000 cP at 160 rpm at 20 deg C. Setting-time data are provided for steel, EPDM, ABS, and beech wood.

Key features

  • Surface-insensitive fast bonding: The ethyl cyanoacrylate bonds acidic and porous materials including wood, leather, cardboard, and paper.
  • Thixotropic vertical control: The gel remains in place on vertical surfaces during application.
  • Very high-viscosity gap filling: The rheology supports gap-filling bonds where a low-flow adhesive is required.

Applications / Suitable for

  • Bonding wood, leather, cardboard, and paper
  • Vertical-surface cyanoacrylate bonding
  • Gap-filling bonds on supported substrates

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
colorless, transparent
Density (g)
1.08 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
80 °C
Other Properties
Storage Temperature
20 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured monomer properties at 20 deg C unless noted; values are not specifications.

Property Value Unit Method / condition
Base compound Ethyl-2-cyanoacrylate Uncured monomer
Appearance Colorless, transparent Uncured monomer
Density 1.08 g/cm^3 20 deg C
Flash point 80 deg C Uncured monomer
Shelf life 12 months Unopened at 20 deg C
Viscosity 35,000-60,000 cP Cone-and-plate, 0.5 rpm at 20 deg C
Viscosity 3,000-6,000 cP Cone-and-plate, 160 rpm at 20 deg C
Technical properties

After-processing / final-state properties

Cured polymer and bonded-substrate properties under the stated stated conditions.

Property Value Unit Method / condition
Cured polymer appearance Transparent Polymer
Service temperature range -55 to 95 deg C Cured polymer
Bond strength on NBR rubber 5-12 N/mm^2 Cured adhesive; material failure indicated
Bond strength on steel 8-17 N/mm^2 Cured adhesive