CYBERBOND 2150

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 2150

Main features

  • High-Viscosity Bead Placement
  • Small-Gap Joint Filling
  • Single-Component Rapid Bonding

Product Description

Cyberbond 2150 provides a high-viscosity cyanoacrylate option for general-purpose bonding where a thicker material is needed. Its liquid profile supports controlled bead placement and helps retain adhesive in small gaps and less closely fitted joints. The product requires no mixing and is used for rapid assembly with compatible substrates. Cyberbond 2150 is suited to applications where localized adhesive placement and small-gap retention are important, including joints that need added adhesive body during rapid assembly.

Key features

  • High-viscosity bead placement: The thicker liquid supports controlled application at the bond line.
  • Small-gap joint filling: The product is used where less closely fitted parts require added adhesive body.
  • Single-component rapid bonding: Its one-part format supports fast application without component mixing.

Applications / Suitable for

  • General-purpose high-viscosity bonding
  • Small gaps and less closely fitted joints
  • Controlled bead application for rapid assembly

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Density (g)
1.06 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
85 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1800 +/- 300 mPa.s
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
Storage Temperature
20 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values. Values are not specifications.

Property Value Unit Method / condition
Technology / base Ethyl Cyanoacrylate
Components One component Ready-to-use liquid
Cure initiation Humidity Cyanoacrylate cure mechanism
Appearance / consistency Clear liquid As supplied
Viscosity 1800 +/- 300 cP Typical product value
Specific gravity 1.06 Typical product value
Flash point 85 deg C 185 deg F
Shelf life 12 months Unopened original container; store 15.5 to 25 deg C