COOLTHERM SC-6702

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6702

Main features

  • 0.7 W/(m K) Silicone Encapsulation
  • 4-Hour Working Life
  • -55 to 260 deg C Material Use

Product Description

CoolTherm® SC-6702 Thermally Conductive Silicone Encapsulant is a two-component silicone system for thermally conductive encapsulation of sensitive electronic modules. The red resin and white hardener mix at a simple 1:1 ratio by weight or volume to form a red material with a typical 30,000 cP viscosity at 25°C, four-hour working life at 25°C, and 25-minute gel time at 66°C. The documented cure is 16–24 hours at 85°C. Typical cured properties include 0.7 W/m·K thermal conductivity, 65 Shore A hardness, 17.1 kV/mm dielectric strength, and an operating-temperature range from -55°C to 260°C.

Key features

  • Two-component thermally conductive silicone encapsulant
  • Simple 1:1 mix ratio by weight or volume
  • 30,000 cP mixed viscosity for cartridge or meter/mix/dispense application
  • Primerless adhesion in most applications, subject to substrate validation
  • Typical 0.7 W/m·K thermal conductivity and 17.1 kV/mm dielectric strength
  • Documented -55°C to 260°C material-use range
  • UL 94 V-0 certified, subject to the current listed formulation and test construction

Applications

  • Thermally conductive encapsulation of sensitive electronic modules
  • Electrical and electronic assemblies requiring flexible silicone insulation
  • High-voltage or critical assemblies using validated vacuum-assisted void control
  • Modules exposed to broad operating temperatures within the documented material-use range

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Resin (A): Red Liq | Hardener (B): White Liq | Mixed: Red Liq
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
A: 2.15 | B: 2.04 | Mixed: 2.09
Physical Properties
Viscosity (Part A)
27000 mPa.s
Viscosity (Part B)
28000 mPa.s
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.7 W/m.K
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
80 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
17.1 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.7 x 10^15 Ohms⋅cm

Additional Information

Thermally conductive silicone encapsulation

CoolTherm® SC-6702 Thermally Conductive Silicone Encapsulant

A two-component silicone system designed to provide heat dissipation and electrical insulation when encapsulating sensitive electronic modules. The material combines a 1:1 mix ratio, moderate mixed viscosity, primerless adhesion positioning, flexible cured properties, and a broad documented material-use temperature range.

Two-component silicone 1:1 weight or volume 30,000 cP mixed 0.7 W/m·K -55°C to 260°C
CoolTherm SC-6702 silicone encapsulant resin and hardener packaging

CoolTherm SC-6702 silicone encapsulant resin and hardener 

As supplied and mixed

Component and mixed-material properties

Thoroughly premix each component before combining the red resin and white hardener at 1:1 by weight or volume.

Property SC-6702 resin SC-6702 hardener Mixed material
Appearance Red liquid White liquid Red liquid
Viscosity at 25°C 27,000 cP 28,000 cP 30,000 cP
Specific gravity 2.15 2.04 2.09
Mix ratio 1:1 by weight or volume
Gel time at 66°C 25 minutes
Working life at 25°C 4 hours
Processing

Premix both components, combine 1:1, minimise air, dispense, and heat cure

Mix the resin and hardener separately before combining them at 1:1 by weight or volume. Automatic meter/mix/dispense equipment may be used for higher-volume production.

  • Use closed-chamber mechanical mixing where practical to reduce introduced air.
  • For extremely high-voltage or other critical applications, evaluate vacuum processing to minimise bubbles and voids.
  • Apply using handheld cartridges or automatic meter/mix/dispense equipment.
  • Avoid surfaces containing cure-inhibiting amines, sulphur, or butyl-containing materials.
  • When substrate compatibility is uncertain, apply a test patch and allow the normal cure time.
  • Cure for 16–24 hours at 85°C after the material reaches the target temperature.
CoolTherm SC-6702 process showing component premixing, one-to-one mixing, optional vacuum de-airing, dispensing, cure-inhibition testing and 85 degree Celsius cure

CoolTherm SC-6702 process showing component premixing, one-to-one mixing, optional vacuum de-airing, dispensing, cure-inhibition testing and 85 degree Celsius cure

1. Premix components

Restore both resin and hardener to a uniform state before metering.

2. Meter and mix

Combine 1:1 by weight or volume and mix thoroughly.

3. Control air and inhibition

Minimise voids and verify uncertain surfaces with a cured test patch.

4. Dispense and cure

Apply the validated fill pattern and hold at 85°C for 16–24 hours after reaching temperature.

Storage and industrial handling

Each component has a six-month shelf life when stored at temperatures up to 40°C in its original unopened container. Keep containers closed, upright, and in well-ventilated storage. The current hardener SDS classifies the material for suspected reproductive toxicity and aquatic hazards, while the resin SDS includes chronic methylpolysiloxane decomposition warnings. Both SDS documents note that formaldehyde may be generated at approximately 150°C and above in oxygen-containing atmospheres. Use trained industrial personnel, adequate ventilation, suitable gloves and eye protection, environmental controls, and current regional SDS and label instructions.

Final cured state

Thermal, mechanical, and electrical properties

The following values are typical cured-material results and are not lot specifications. Installed thermal and electrical performance also depends on geometry, thickness, coverage, interfaces, voids, cure, voltage design, and the surrounding assembly.

Property Typical value Context
Thermal conductivity 0.7 W/m·K Hot Disc Transient Method, ISO 22007-2.
Coefficient of linear thermal expansion 239 ppm/°C ASTM C864.
Hardness 65 Shore A Flexible cured silicone.
Tensile strength 4.1 MPa (600 psi) ASTM D412 bulk-material property.
Elongation at break 80% ASTM D412.
Volume resistivity at 25°C 1.7 × 1015 ohm-cm ASTM D257; not a finished-assembly working-voltage rating.
Dielectric strength 17.1 kV/mm (434 V/mil) ASTM D149; breakdown property rather than design working voltage.
Dielectric constant 5.5 at 1 MHz and 25°C ASTM D150.
Dissipation factor 0.014% at 1 MHz and 25°C ASTM D150 as published in DS3567.
Applications and design considerations

Thermal encapsulation for sensitive electronic modules

SC-6702 is directly positioned for encapsulating sensitive electronic modules where heat dissipation, electrical insulation, flexible silicone properties, and broad-temperature capability are required. Final selection must consider component layout, fill depth, void tolerance, cure inhibition, voltage, creepage and clearance, thermal path, enclosure design, repairability, and environmental exposure.

Sensitive electronic module encapsulated with red thermally conductive silicone

Sensitive electronic modules

Designed to combine thermal conduction and electrical insulation around sensitive components and interconnects.

High-voltage electronic assembly using vacuum-assisted silicone encapsulation

Critical and high-voltage assemblies

Vacuum processing may be evaluated when bubbles and voids could affect electrical performance.

Electronic module operating across a broad temperature range with silicone encapsulation

Broad-temperature modules

The material is documented for parts and devices operating from -55°C to 260°C, subject to application-level validation.

Validate SC-6702 for your electronic encapsulation process

Krayden can help review mix-ratio control, component premixing, meter/mix/dispense equipment, vacuum processing, cure inhibition, fill geometry, void control, cure profile, thermal path, electrical insulation, operating temperature, UL scope, and assembly-level qualification for CoolTherm® SC-6702.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers