COOLTHERM MG-121

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

COOLTHERM MG-121

Main features

  • 2.3 W/(m K) Thermal Conductivity
  • Low-Modulus Cured Bonding
  • Eight-Hour Working Window

Product Description

CoolTherm® MG-121 Thermally Conductive Gel is a one-component silicone thermal interface material for transferring heat from flip-chip microprocessors, PPGAs, BGAs, microBGAs, DSPs, graphics accelerator chips, and other high-wattage electronic components. The grey paste has a typical viscosity of 60,500 cP at 20 rpm or 75,000 cP at 10 rpm at 25°C, an eight-hour working life at 25°C, and an eight-minute gel time at 100°C. It is formulated for 1–2 mil thin bondlines and to inhibit bleed, separation, and pump-out. Supported cure schedules are 2 hours at 100°C, 60 minutes at 125°C, or 30 minutes at 150°C. Typical cured properties include 2.3 W/m·K thermal conductivity, 30,000 Pa storage modulus at 25°C, -121°C Tg, and 8 × 1013 ohm-cm volume resistivity.

Key features

  • One-component silicone gel for high-wattage semiconductor thermal interfaces
  • Designed for 1–2 mil thin bondlines
  • 2.3 W/m·K typical thermal conductivity
  • Formulated to inhibit bleed, separation, and pump-out
  • Low 30,000 Pa storage modulus at 25°C and -121°C Tg
  • Positioned for HAST, moisture, and temperature-cycling resistance
  • UL 94 V-0 certified, subject to the current listed formulation and test construction

Applications

  • Flip-chip microprocessors
  • PGA, BGA, and microBGA packages
  • DSP and graphics accelerator chips
  • Other high-wattage electronic components requiring a cured, compliant thermal interface

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray Paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
8
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
20 rpm: 60500 | 10 rpm: 75000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-121 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
2.3 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
8 x 10^13 Ohms⋅cm

Additional Information

Cured silicone thermal interface gel

CoolTherm® MG-121 Thermally Conductive Gel

A one-component silicone interface material engineered to transfer heat from flip-chip microprocessors and other high-wattage semiconductor packages. MG-121 is formulated for thin 1–2 mil bondlines, good wetting, low cured modulus, and resistance positioning against bleed, separation, pump-out, moisture, and temperature cycling.

One-component silicone gel 1–2 mil bondline 2.3 W/m·K 8-hour working life UL 94 V-0
CoolTherm MG-121 thermally conductive gel syringe packaging

CoolTherm MG-121 thermally conductive gel 

As supplied

Frozen, syringe-dispensable gel properties

MG-121 is supplied as a grey paste. The datasheet reports two viscosity values at different rotational speeds, so the speed condition remains attached to each result.

Property Typical value Context
Appearance Grey paste One-component silicone thermal gel.
Viscosity at 25°C, 20 rpm 60,500 cP Speed-specific TDS value.
Viscosity at 25°C, 10 rpm 75,000 cP Speed-specific TDS value.
Specific gravity 2.56 Consistent with the current SDS density of 2.56 g/cm³.
Gel time at 100°C 8 minutes Gel time is not equivalent to the full cure schedule.
Working life at 25°C 8 hours Ambient process window after thawing and conditioning.
Processing

Thaw upright, dry and purge the syringe, dispense the controlled interface, and heat cure

Warm the frozen syringe naturally to room temperature, ideally 20–25°C, while keeping it vertical with the dispense tip facing downward. Do not use ovens, hot plates, hot-air guns, warm water, or other artificial heat sources to accelerate thawing.

  • Typical thaw time from -30°C to 25°C is 75 minutes for a 3–10 cc syringe, 1.5 hours for a 30–55 cc syringe, and two hours for a six-ounce cartridge.
  • Remove surface moisture before use and manually purge normal tip-area air.
  • Mount the syringe on thoroughly cleaned dispensing equipment and purge until the flow is unbroken.
  • Control dispense volume, coverage, pressure, bondline stops, assembly force, and final 1–2 mil bondline through the validated part design.
  • Cure for two hours at 100°C, 60 minutes at 125°C, or 30 minutes at 150°C.
  • Count cure time after the gel reaches the target temperature and account for oven ramp and assembly thermal mass.
CoolTherm MG-121 process showing upright frozen storage, ambient thawing, moisture removal, syringe purging, controlled dispensing, thin bondline assembly and cure

CoolTherm MG-121 process showing upright frozen storage, ambient thawing, moisture removal, syringe purging, controlled dispensing, thin bondline assembly and cure

1. Thaw upright

Allow the frozen syringe to reach 20–25°C naturally with the tip facing down.

2. Dry and purge

Remove condensation and purge syringe-tip air and the dispensing path.

3. Dispense and assemble

Apply the validated pattern and compress to the controlled 1–2 mil bondline.

4. Heat cure

Use the 100°C, 125°C, or 150°C time-at-temperature schedule.

Frozen storage and industrial handling

Shelf life is six months when stored at -30°C in the original unopened container. Store syringes vertically with the dispense tip facing downward and do not store them horizontally. The material crystallises at -40°C, so avoid storage at -40°C or below. The current US SDS is effective 1 November 2024 and identifies inhalation, reproductive, and aquatic hazards. It also notes that methylpolysiloxanes may generate formaldehyde at approximately 150°C and above in oxygen-containing atmospheres. Use trained industrial personnel, adequate ventilation, suitable gloves and eye protection, environmental controls, and the current regional SDS and label.

Final cured state

Thermal, mechanical, expansion, and electrical properties

The following values are typical cured-material properties. Thermal conductivity does not by itself define installed thermal resistance; the final interface also depends on bondline thickness, contact quality, area, pressure, flatness, cure, and adjacent surfaces.

Property Typical value Context
Thermal conductivity 2.3 W/m·K Hot Disc Transient Method, ISO 22007-2.
Coefficient of linear thermal expansion 232 ppm/°C α2 Only the α2 value is published in DS3661.
Glass transition temperature -121°C By TMA.
Storage modulus at 25°C 30,000 Pa Low-modulus cured gel property.
Volume resistivity at 25°C 8 × 1013 ohm-cm Bulk electrical property; not an assembly working-voltage rating.
Applications and interface design

Thin-bondline thermal coupling for high-wattage semiconductor packages

MG-121 is directly positioned for transferring heat from flip-chip microprocessors, PPGAs, BGAs, microBGAs, DSP chips, graphics accelerator chips, and other high-wattage components. Selection requires validation of the actual heat load, area, bondline, clamping or assembly force, surface flatness, material coverage, cure, electrical clearances, rework method, and environmental profile.

Flip-chip microprocessor coupled to a heat spreader using a thin cured thermal gel bondline

Flip-chip microprocessors

Designed for efficient heat transfer through a controlled 1–2 mil cured gel interface.

BGA and microBGA semiconductor packages using compliant thermal interface gel

PGA, BGA, and microBGA packages

Low cured modulus supports compliant thermal coupling, subject to the package and mechanical design.

DSP and graphics accelerator chips thermally coupled using silicone gel

DSP and graphics devices

Suitable for evaluation in high-wattage digital and graphics devices requiring a cured thermal interface.

Product catalogue

Microelectronic Materials Catalogue — PC3003

The catalogue lists MG-121 as a one-component thermally conductive gel with 60,500 cP viscosity, the three supported cure schedules, 2.3 W/m·K conductivity, 8 × 1013 ohm-cm resistivity, -121°C Tg, and bleed, separation, pump-out, and HAST-resistance positioning.

Open the Microelectronic Materials Catalogue
User instructions

Electronic Materials Handling — -30°C Storage

UI3027 provides frozen-storage orientation, insulated-glove guidance, FIFO handling, ambient thawing, package-specific thaw times, condensation removal, and tip-purging instructions.

Open the -30°C handling instructions
Selector guide

Electronic Materials for LED Applications — SG1013

The LED selector guide includes MG-121 in its thermal-material comparison table with silicone chemistry, UL 94 V-0, 60,500 cP viscosity, 2.3 W/m·K conductivity, six-month shelf life at -30°C, eight-hour working life, and the documented cure schedules.

Open the LED Materials Selector Guide

Validate MG-121 for your semiconductor thermal interface

Krayden can help review heat load, interface area, 1–2 mil bondline control, dispense pattern, frozen handling, assembly pressure, surface flatness, cure profile, HAST and thermal-cycling requirements, rework, UL scope, and assembly-level thermal resistance for CoolTherm® MG-121.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers