COOLTHERM ES-40

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM ES-40

Main features

  • Eight Configurable Hardener Options
  • Adhesive, Laminating, and Electrical-Insulation Uses
  • Up to 77.2 MPa Tensile Strength

Product Description

Thermoset® ES-40 Epoxy System is a white, unfilled, general-purpose epoxy resin platform used with Thermoset® Hardeners No. 18, 25, 37, 65, 66, 67, 70, or 71. Hardener selection changes the mixed ratio, working life, cure schedule, rigidity, flexibility, heat resistance, moisture response, appearance, and cured electrical and mechanical properties. The resin has a typical 14,000 cP viscosity at 25°C and 1.18 specific gravity. Supported systems provide working lives from 5 to 75 minutes for a 200 g mass and room-temperature or elevated-temperature cure. Typical cured hardness ranges from 60 to 92 Shore D, tensile strength from 15.9 to 77.2 MPa, and elongation at break from 3.5% to 55%, depending on the selected hardener and ratio.

Key features

  • Eight supported hardener options for different processing and cured-property requirements
  • General-purpose resin for adhesive, laminating, and electrical or electronic insulation applications
  • Room-temperature and elevated-temperature cure options
  • Typical cured hardness from 60 to 92 Shore D
  • Typical tensile strength from 15.9 to 77.2 MPa
  • Adjustable rigid-to-flexible behaviour with selected hardeners and documented variable mix ratios
  • Six-month resin shelf life at 25°C in the original unopened container

Applications

  • Electrical and electronic insulation, potting, and encapsulation
  • General-purpose adhesive bonding
  • Laminating and cast parts requiring hardener-selectable rigidity or flexibility
Product Family

COOLTHERM ES-40

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.18
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
14000 mPa.s

Additional Information

Configurable general-purpose epoxy platform

Thermoset® ES-40 Epoxy System

A white, unfilled epoxy resin formulated for use with eight Thermoset® hardeners. The selected hardener controls handling, cure, rigidity, flexibility, appearance, heat resistance, environmental response, and final electrical and mechanical properties for adhesive, laminating, and electrical or electronic insulation applications.

White unfilled resin Eight hardener options 14,000 cP resin 5–75 min working life 25°C or heat cure
Thermoset ES-40 epoxy resin with compatible Thermoset hardener packaging

Thermoset ES-40 epoxy resin with compatible Thermoset hardener 

As supplied

ES-40 resin properties

ES-40 is supplied as a white unfilled liquid resin. Mixed-system properties depend on the hardener and ratio selected.

Property Typical value Context
Appearance White liquid Unfilled epoxy resin.
Viscosity at 25°C 14,000 cP Resin-only value; mixed viscosity is hardener-dependent.
Specific gravity 1.18 Typical as-supplied resin value.
Variant comparison

Select the hardener for the required process and final material

The hardeners are separate formulations. Mix ratios, working lives, cure schedules, compliance language, and final properties must remain tied to the selected system.

Field No. 18 No. 25 No. 37 No. 65 No. 66 No. 67 No. 70 No. 71
Primary positioning Heat-resistant room-temperature system Fast room-temperature cure; high-gloss finish Variable flexibility; conditional food-contact formulation Low-viscosity, high-gloss encapsulation Low-stress, variable rigidity Elevated-temperature cure; up to 155°C continuous operation Low-viscosity, impact and thermal-shock resistance Low-exotherm, semi-rigid flexible system
Mix ratio by weight 100:14 100:100 100:100* 100:40 100:50* 100:24 100:30 100:100
Mix ratio by volume 100:16 100:122 100:120 100:50 100:60* 100:30 100:35 100:120
Working life, 200 g at 25°C 20 min 5 min 75 min 50 min 60 min 60 min 30 min 60 min
Cure schedule 24 h at 25°C 24 h at 25°C 24 h at 25°C; 2 h at 66°C; or 0.05 h at 93°C 24 h at 25°C 24 h at 25°C 2 h at 100°C; optional 2 h at 150°C 24 h at 25°C 24 h at 25°C

*Hardener No. 37 and No. 66 ratios may be varied to change bond rigidity. Food-contact compliance for No. 37 requires exactly 100 parts resin to 54 parts hardener by weight and compliance with all stated proportioning, mixing, application, and cure conditions.

Processing

Meter the selected hardener, minimise air, dispense, and follow its cure schedule

Transfer the required quantity of ES-40 resin to a clean container and add the selected hardener at its documented ratio. Mix thoroughly until uniform. Automatic meter/mix/dispense equipment may be used for higher-volume production.

  • Minimise entrapped air during mixing.
  • For high-voltage or other critical electrical applications, vacuum processing may be appropriate to reduce bubbles and voids.
  • Apply using validated automatic meter/mix/dispense equipment.
  • Follow only the cure schedule for the selected hardener.
  • Start cure timing after the material reaches the stated temperature and account for oven ramp and part thermal mass.
Thermoset ES-40 process showing hardener selection, ratio control, mixing, optional vacuum de-airing, dispensing and cure

Thermoset ES-40 process dispensing and cure

Storage and handling

ES-40 resin has a six-month shelf life when stored at 25°C in its original unopened container. If crystals form after cool storage or shipment, gently warm the resin to 50–60°C until the crystals melt before adding hardener. Use disposable mixing equipment where practical; solvent-cleaned equipment must be fully dry before reuse. Review the current resin and selected-hardener SDS and labels before handling.

Final cured state

Hardener-specific mechanical and electrical properties

The typical properties below apply only to the stated ES-40/hardener formulation and test condition. Variable-ratio systems can produce different results.

Property No. 18 No. 25 No. 37 No. 65 No. 66 No. 67 No. 70 No. 71
Hardness, Shore D 88 80 84 85 85 92 82 60
Tensile strength, MPa 77.2 56.5 51.7 62.1 52.4 75.2 59.6 15.9
Elongation at break, % 3.6 5 4.5 4.5 12 5.2 3.5 55
Moisture absorption, 24 h at 25°C, % 0.18 0.23 0.55 0.22 0.35 0.20 0.36 0.85
Volume resistivity at 25°C, ohm-cm 4 × 1016 2.4 × 1014 1 × 1016 1 × 1015 1 × 1016 1 × 1016 2 × 1016 1 × 1014
Dielectric constant, 1 MHz at 25°C 3.8 3.4 3.7 4.2 3.7 4.4 3.4 4.2
Dissipation factor, 1 MHz at 25°C 0.020 0.028 0.016 0.016 0.016 0.038 0.025 0.021
Applications

Adhesive, laminating, and electrical-insulation uses

ES-40 is directly positioned for adhesive, laminating, and electrical or electronic insulation. Application selection must include the exact hardener, ratio, cure schedule, desired rigidity, voltage, geometry, humidity, operating temperature, and substrate.

Electronic assembly potted with white general-purpose epoxy system

Electrical and electronic insulation

Suitable for potting, encapsulation, and insulation where the selected hardener’s electrical and mechanical properties fit the design.

General-purpose adhesive joint bonded using Thermoset ES-40 epoxy

Adhesive bonding

Hardener No. 37 and No. 66 provide documented ratio-dependent rigidity, while the other hardeners offer additional heat, appearance, or environmental profiles.

Laminated composite or cast part produced with white epoxy resin

Laminating and cast parts

The unfilled resin platform supports laminating and casting where selectable viscosity, cure, stiffness, or flexibility is required.

Product resource

Potting & Encapsulation Materials Catalogue — PC3002

The catalogue provides portfolio-level comparison and lists the ES-40/70 system as a white, unfilled, moderate-viscosity two-component epoxy with 550 cP mixed viscosity, a 100:30 weight ratio, 24-hour room-temperature cure, and 82 Shore D hardness.

The current ES-40 technical datasheet governs the complete eight-hardener platform. Use catalogue values only for the identified ES-40/70 combination.

Open the Potting & Encapsulation Materials Catalogue

Select the ES-40 hardener for your process and final property requirements

Krayden can help review hardener selection, mix-ratio control, working life, vacuum processing, dispensing, cure schedule, rigidity, flexibility, heat resistance, electrical properties, moisture exposure, and application qualification for Thermoset® ES-40.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services