COOLTHERM EP-6007

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-6007

Main features

  • 45-Minute Working Window
  • 0.62 W/(m K) Thermal Interface
  • 19.7 kV/mm Dielectric Strength

Product Description

CoolTherm® EP-6007 BLK Epoxy Resin is a black, ceramic-filled epoxy resin formulated for use with CoolTherm® EP-6010 Hardener, Thermoset™ Hardener No. 67, or CoolTherm® EP-6252 Hardener. The resulting two-component systems are suitable for thermally conductive potting and casting and for thin-bondline attachment of semiconductors to heat sinks. Depending on the selected hardener, the cured system provides a typical thermal conductivity of 0.50–0.62 W/m·K, dielectric strength of 18.8–19.7 kV/mm, and operating-temperature capability from -55 to 130 °C.

Key features

  • Thermally conductive epoxy system: Provides a typical cured thermal conductivity of 0.50–0.62 W/m·K, depending on the selected hardener.
  • Electrical insulation: Delivers typical dielectric strength of 18.8–19.7 kV/mm and volume resistivity up to 2 × 1016 ohm-cm.
  • Configurable processing: Supported hardener options provide working lives from 45 minutes to 8 hours at 25 °C and multiple room-temperature or heat-cure schedules.

Applications / Suitable for

  • Thermally conductive potting and casting
  • Thin-bondline attachment of semiconductors to heat sinks
  • Applications requiring electrical insulation and non-burning properties

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.69
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
15000 mPa.s
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.5 - 0.62 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm EP-6007 BLK resin and its mixed systems before cure. Mix ratio, working life, and cure schedule depend on the selected hardener. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid — CoolTherm EP-6007 BLK resin as supplied
Viscosity 15,000 cP Resin at 25 °C; test method not stated
Specific gravity 1.69 — Resin; test temperature and method not stated
Mix ratio by weight 100:5.5 / 100:9 / 100:10 Resin:hardener EP-6010 Hardener / Thermoset Hardener No. 67 / EP-6252 Hardener
Working life 2 / 8 / 45 hours / hours / minutes At 25 °C; EP-6010 Hardener / Thermoset Hardener No. 67 / EP-6252 Hardener
Cure time — EP-6010 Hardener 12–16 hours At 25 °C
Cure time — Thermoset Hardener No. 67 16 / 5 / 3 hours At 65 / 100 / 130 °C; suitable for pourings up to 227 g in a concentrated mass
Cure time — EP-6252 Hardener 24 / 1 hours At 25 / 65 °C
Shelf life 1 year Stored at 25 °C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm EP-6007 BLK systems with EP-6010 Hardener, Thermoset Hardener No. 67, or EP-6252 Hardener. Values are listed in that order and are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 0.60 / 0.50 / 0.62 W/m·K Hot Disc Transient Method, ISO 22007-2
Coefficient of thermal expansion, α1 47 / 42 / 36 ppm/°C Temperature region and test method not stated
Coefficient of thermal expansion, α2 122 / 140 / 161 ppm/°C Temperature region and test method not stated
Glass transition temperature 54 / 94 / 45 °C TMA
Hardness 85 / 85 / 83 Shore D EP-6010 Hardener / Thermoset Hardener No. 67 / EP-6252 Hardener
Tensile strength at 25 °C 57 (8,400) / 67 (9,800) / 22 (3,200) MPa (psi) Test method not stated
Elongation at yield 0.7 / 1.2 / 1.4 % Test method not stated
Moisture absorption 0.4 / 0.4 / 0.8 % 10 days at 25 °C; exposure medium and test method not stated
Linear shrinkage 0.002 / 0.003 / 0.009 in/in Test method and cure condition not stated
Volume resistivity at 25 °C 2 × 1016 / 2 × 1016 / 1 × 1014 ohm-cm Test method not stated
Dielectric strength 19.3 (490) / 19.7 (500) / 18.8 (477) kV/mm (V/mil) ASTM D149
Dielectric constant 4.3 / 4.4 / 3.7 — At 25 °C and 125 kHz; ASTM D150
Dissipation factor 0.020 / 0.020 / 0.024 — At 25 °C and 100 kHz; ASTM D150

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers